Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 49 g/10 min @Load 5.00 kg, Temperature 230 °C |
49 g/10 min @Load 11.0 lb, Temperature 446 °F |
|
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Melt Flow | 49 g/10 min @Load 5.00 kg, Temperature 300 °C |
49 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 49 g/10 min @Load 5.00 kg, Temperature 300 °C |
49 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Asia Pacific) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 49 g/10 min @Load 5.00 kg, Temperature 300 °C |
49 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL V03505 PPE+HIPS (Europe-Africa-Middle East) Noryl* V03505 is a 35% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Melt Flow | 49 g/10 min @Load 10.0 kg, Temperature 250 °C |
49 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 49 g/10 min @Load 10.0 kg, Temperature 250 °C |
49 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HA-1011 PC/ABS, Unreinforced Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 49 g/10 min @Load 1.20 kg, Temperature 224 °C |
49 g/10 min @Load 2.65 lb, Temperature 435 °F |
ASTM D1238 |
Lubrizol Estane® 2102-65D Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Melt Flow | 49 g/10 min @Load 10.0 kg, Temperature 190 °C |
49 g/10 min @Load 22.0 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® FK 66003 20% Silicone Filled POM Description: Polyoxymethylene based batch with approx. 20% silicone (polysiloxane) for modifying tribological properties of thermoplastic polyoxymethylenes. Recommended concentrations of batch FK660.. |
|||
Melt Flow | 49 g/10 min @Load 5.00 kg, Temperature 270 °C |
49 g/10 min @Load 11.0 lb, Temperature 518 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Pocan® S 7020 000000 PBT PBT, non-reinforced, injection molding, extrusion, flame retardant, impact modified |