Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.2 g/10 min | 4.2 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE G 7155 BLK Multi-Flex® G 7155 is based on Shell's Kraton G technology, manufactured under the license of Shell. Multibase certifies that his product has been formulated with the same ingredients as manufactu.. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
Procedure A Condition E; ASTM D1238 |
Network Polymers NPP 50-0350 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
NOVA Chemicals Novapol® TF-0438-E Hexene LMDPE Film Resin TF-0438-E complies with the U.S. FDA specifications for olefin polymers and may be used in the U.S. as an article or component of an article intended for use in contact with food, without temperatur.. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg |
4.2 g/10 min @Load 4.76 lb |
ASTM D1238 |
Reliance Industries Reclair R35042 Polyethylene Rotational molding Medium Density Polyethylene grade. Characteristics:good toughness, good impact resistance, good environmental stress crack resistance. Applications:chemical tanks, water storage .. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH042V Polypropylene, Homopolymer, Extrusion, Sheet COPYLENE™ CH042V is a polypropylene homopolymer resin often used in extrusion applications. Replacement alternative to Pro-fax® HL561KInformation provided by Phillips 66. |
|||
Melt Flow | 4.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
cm³/10 min |
Polimeri Europa EDISTIR SRL800/N High Impact Polystyrene (HIPS)
(discontinued **) Symbol according to ISO 1043-1: S/B Designation: Thermoplastic ISO 2897-SB,G,093-06-07-12 Very high environmental stress cracking resistant (VH ESCR) modified HIPS. It exhibits high toughness and .. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman 1924P Polyethylene
(discontinued **) Low-density polyethylene 1924P is a resin in the boardstock coating industry for use in breadboard, cupstock, and liquid packaging board. This material has an excellent combination of low neck-in, .. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH042L Polypropylene, Homopolymer, Straw and Extrusion, Antistat COPYLENE™ CH042L is specifically designed for application in extrusion applications such as straws. Applications: Straws.Information provided by Phillips 66. |
|||
Melt Flow | 4.2 g/10 min | 4.2 g/10 min | ASTM D1238 |
Flint Hills P4G2T-077D Homopolymer Polypropylene Homopolymer, FDA compliantFeatures: Antistat.Applications: Extrusion: straw grade.Former Huntsman polypropylene products are now produced by Flint Hills Resources. |
|||
Melt Flow | 4.2 g/10 min | 4.2 g/10 min | ASTM D1238 |
Flint Hills P4G3Z-050F Polypropylene Homopolymer Features: Low Water Carry-over, good film quality. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: cast filmInformation Provided by Flint Hills Resource.. |
|||
Melt Flow | 4.2 g/10 min @Load 3.80 kg, Temperature 230 °C |
4.2 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical LUPOS GP2100 ABS+GF10%, General Purpose Feature: Injection Molding, ABS+GF10%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9, 9003-54-7 and 65997-17-3Information provided by LG Chemical |
|||
Melt Flow | 4.2 g/10 min @Load 6.60 kg, Temperature 337 °C |
4.2 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2400 PEI 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors. |
|||
Melt Flow | 4.2 g/10 min @Load 6.60 kg, Temperature 337 °C |
4.2 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 2400 PEI (Asia Pacific) 40% Glass fiber filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. WRAS certification in recognized colors. |
|||
Melt Flow | 4.2 g/10 min @Load 6.60 kg, Temperature 337 °C |
4.2 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AR9300 PEI 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 4.2 g/10 min @Load 6.60 kg, Temperature 337 °C |
4.2 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AR9300 PEI (Asia Pacific) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Melt Flow | 4.2 g/10 min @Load 6.60 kg, Temperature 337 °C |
4.2 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5001 PEI Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Melt Flow | 4.2 g/10 min @Load 6.60 kg, Temperature 337 °C |
4.2 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Asia Pacific) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
Melt Flow | 4.2 g/10 min @Load 1.00 kg, Temperature 190 °C |
4.2 g/10 min @Load 2.20 lb, Temperature 374 °F |
ASTM D1238R |
UBE 7128B Nylon 6/12 Copolymer Description: UBESTA Nylon 12 CopolymerInformation provided by UBE. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Unipetrol PE HD LITEN® MS 57 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Melt Flow | 4.2 g/10 min | 4.2 g/10 min | ASTM D1238 |
Westlake Mxsite LC78104 Polyethylene Mxsite LC78104 polyethylene is recommended for the skin layers of cast stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling .. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Appeel® 45D747 Polyolefin Appeel® 45D747 is a modified polyolefin resin designed to provide easy peel functionality from polyethylene copolymers. Appeel® 45D747 is available in pellet form for use in conventional extrusion.. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238, ISO 1133 |
DuPont™ Bynel® 41E755 Anhydride Modified LLDPE BYNEL® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal.. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 201.48 Low Density Polyethylene Resin Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal.. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem D040A Homopolymer Polypropylene Description: Injection Molding, Wet and Dry Long-Term Heat AgingApplications: Suggested Uses Include Appliance, Containers, Closures, HousewaresThis resin meets the requirements for olefin polymers .. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem D042M Homopolymer Polypropylene Description: Injection Molding, General Purpose, Low Water Carryover, UV ResistantApplications: Suggested Uses Include Tape, Slit-film Fibers, Containers, Closures, HousewaresThis resin meets the re.. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM-D1238 |
Braskem RA34U3 LLDPE Rotomolding Polyethylene The resin RA34U3 is a linear low-density polyethylene, 1-butene based, with a good balance of processability, environmental stress cracking resistance, and impact strength. It contains long term UV6.. |
|||
Melt Flow | 4.2 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.2 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
ExxonMobil PP2252E4 Homopolymer Product Description: Medium melt flow rate homopolymer designed for high speed extrusion of woven fabrics exhibiting low water carry over.Availability: North America and South America Features:Bal.. |