Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Europe-Africa-Middle East) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Melt Flow | 30 - 45 g/10 min @Load 2.16 kg, Temperature 250 °C |
30 - 45 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
PTS PBT-1100 PBT Resin Information provided by PTS LLC. |
|||
Melt Flow | 30 g/10 min | 30 g/10 min | ISO 1133 |
Solvay Engineered Polymers SEQUEL® 2330 Engineered Polyolefin
(discontinued **) Description: SEQUEL® 2330 engineered polyolefin is designed for large mold-in-color automotive interior applications that require stiffness and good dimensional stability. This material exhibits e.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 190 °C |
30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SABIC M300054 High Density Polyethylene for Injection Molding Product Description: M300054 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good flow.. |
|||
Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 220 °C |
30 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AP163 ABS, Permanent Anti-Static Feature: Injection Molding, Permanent Anti-StaticApplication: E & E Products (IC tray etc)CAS No. 9003-56-9Information provided by LG Chemical |
|||
Melt Flow | 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Kotec Carbotex K-20UV30 Polycarbonate, General Purpose, UV Stability Grade UV stability, Ultra Low viscosity, TransparentApplications: OA equipment, Communications, Precision parts, Machineries, Lighting covers, Safety products, E & E parts, Household applications, Leisure.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-9120 20% Talc-Filled Polypropylene Block-Copolymer INNOPOL® CS 2-9120 is a 20% talc-filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9120 is developed for producing.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
nozzle diam 2.095 mm; ISO 1133 |
Inno-Comp INNOPOL® CS 3-9120 SR5 17% Talc Filled Polypropylene Blend INNOPOL® CS 3-9120 SR5 is a 17% talc-filled compound based on blend of polypropylene block copolymer and homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 3-9.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Kuraray SEPTON® PM2 Polypropylene Modified Plastic Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 380 °C |
30 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a.. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 250 °C |
30 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® AR-5300H PBT/ASA, 30% Glass Filled Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 250 °C |
30 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® LS-3104G PC, 10% Glass Filled High Impact High-impact resistant PC/GF with 10% GF reinforcement for LCD BLFInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 30 g/10 min @Load 1.20 kg, Temperature 300 °C |
30 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Teijin Panlite® L-1225ZL100 Transparent and Weather Resistant grade Polycarbonate Resin Conforms to SAE regulations. It is a thin wall injection molding grade as it has high fluidity, weather resistance and mold release property and is bluish-tinted to exhibit clear color.Applications:.. |
|||
Melt Flow | 30 g/10 min @Load 10.0 kg, Temperature 220 °C |
30 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Novodur® M210TF ABS Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution |
|||
Melt Flow | 30 - 36 g/10 min @Temperature 230 °C |
30 - 36 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 1930UX Extra High Flow, UV Stabilized Copolymer Polypropylene DescriptionPolyfort® PP 1930UX is an extra high flow, heat resistant, UV stabilized copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis HG313MO Polypropylene HG313MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grad is designed for high-speed inject.. |
|||
Melt Flow | 30 g/10 min @Temperature 230 °C |
30 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 - 35 g/10 min | 30 - 35 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Melt Flow | 30 g/10 min @Temperature 230 °C |
30 g/10 min @Temperature 446 °F |
Condition L; ASTM D1238 |
A. Schulman PP 2175 Polypropylene High Flow Copolymer Polypropylene DescriptionPolypropylene PP 2175 is a high flow copolymer polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 g/10 min @Temperature 230 °C |
30 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 4181T Injection Molding Polypropylene Homopolymer with Antistat, ESCR AdditivesApplications: For general purpose injection molding applications such as closures.Formolene 4181T is a low viscosity, highly isotactic polypropylene homopoly.. |
|||
Melt Flow | 30 - 35 g/10 min | 30 - 35 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Melt Flow | 30 - 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 - 35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman. |
|||
Melt Flow | 30 g/10 min @Load 5.00 kg, Temperature 260 °C |
30 g/10 min @Load 11.0 lb, Temperature 500 °F |
estimated from MVR using room temperature density; ISO 1133 |
Covestro Makroblend® KU 2-7940 Polycarbonate + PBT, Impact Grade Developmental productISO 7792-1-PC/PBT,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 160 °C |
30 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® 9E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 230 °C |
30 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil Exxtral™ BMV 301 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin characterized by a good stiffness/toughness balance, designed for automotive interior application in which good surface finish, high s.. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg |
30 g/10 min @Load 4.76 lb |
Melt flow ratio I10/I2 is 8.5. |
Dow HDPE 30460M High Density Polyethylene DOW HDPE 30460M resin is a medium molecular weight distribution copolymer designed to offer moderate impact strength and stress crack resistance with excellent rigidity. This resin has excellent pro.. |
|||
Melt Flow | 30 g/10 min @Temperature 230 °C |
30 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFORT™ PP 2268UX Heat Resistant Polypropylene DescriptionPolyfort® PP 2268UX is a UV stabilized, extra high flow unique high modulus, heat resistant polypropylene.Information provided by A. Schulman. |
|||
Melt Flow | 30 g/10 min @Load 2.16 kg, Temperature 380 °C |
30 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)
(discontinued **) Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, b.. |