Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 17.8 g/10 min @Load 2.16 kg, Temperature 230 °C |
17.8 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Noble Polymers Ecobarrier™ 0712 Thermoplastic Olefin (TPO) Ecobarrier is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. Ecobarrier is primarily used as a sound barrier material in low heat applications.Informa.. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP COLORCOMP EX12304C PEI (Asia Pacific) LNP* Colorcomp* EX12304C is an unfilled polyetherimide clean compound with extremely high level of cleanliness for the most demanding application. This compound is manufactured using LNP CCS technol.. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010F PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer b.. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010F PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant, NSF 51 listing. Effective June 2007, this grade will no longer be .. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010K PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010K PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010M PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010P PEI Enhanced flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010R PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010TC PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant, NSF 51 listing. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010X PEI Enhanced flow Polyetherimide (Tg 217C) with low ionic contamination of less than 0.1 ppm each of leachable chloride and sulphates. ECO Conforming. Factory Mutual FM4910 compliant in recognized col.. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9011 PEI Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9011 PEI (Asia Pacific) Transparent, high flow Polyetherimide (Tg 217C). ECO Conforming. Improved processability for Fiber extrusion. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 9011 PEI (Europe-Africa-Middle East) Transparent, high flow Polyetherimide (Tg 217C). Resin is RoHS compliant. Improved processability for Fiber extrusion. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM HU1010 PEI Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI),.. |
|||
Melt Flow | 17.8 g/10 min @Load 5.00 kg, Temperature 250 °C |
17.8 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V4860HR PBT 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM AUT200 PEI Transparent high flow Polyetherimide (Tg 217C). Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperat.. |
|||
Melt Flow | 17.8 g/10 min @Load 5.00 kg, Temperature 250 °C |
17.8 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V4860HR PBT (Asia Pacific) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Melt Flow | 17.8 g/10 min @Load 5.00 kg, Temperature 250 °C |
17.8 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Melt Flow | 17.8 g/10 min @Load 6.60 kg, Temperature 337 °C |
17.8 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 1010M PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming. |