Physical Properties Metric English Comments
Melt Flow 12.1 - 18 g/10 min

@Load 1.20 kg,
Temperature 300 °C
12.1 - 18 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Iran Petrochemical (PCC) PC 1218 Polycarbonate
Suitable for molding, injection, and blow moldingInformation provided by Iran Petrochemical Commercial Co.
Melt Flow 12.1 g/10 min

@Load 10.0 kg,
Temperature 230 °C
12.1 g/10 min

@Load 22.0 lb,
Temperature 446 °F
Calculated from Volume Flow Rate of 10.5 cm<sup>3</sup>/10 min; ISO 1133
DSM Arnitel® EB463 41 Shore D, Blow Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melt Flow 12.1 g/10 min

@Load 10.0 kg,
Temperature 230 °C
12.1 g/10 min

@Load 22.0 lb,
Temperature 446 °F
Calculated from Volume Flow Rate of 10.5 cm<sup>3</sup>/10min.; ISO 1133
DSM Arnitel® EB463 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melt Flow 12.1 g/10 min

@Load 10.0 kg,
Temperature 230 °C
12.1 g/10 min

@Load 22.0 lb,
Temperature 446 °F
Calculated from Volume Flow Rate of 10.5 cm<sup>3</sup>/10 min; ISO 1133
DSM Arnitel® EB464 42 Shore D, Blow Molding Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melt Flow 12.1 - 15.3 g/10 min
12.1 - 15.3 g/10 min
Average value: 14.1 g/10 min Grade Count:3
Overview of materials for Polyethersulfone, Carbon Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximu..
Melt Flow 12.1 - 16 g/10 min
12.1 - 16 g/10 min
D
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion
Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff..
Melt Flow 12.1 g/10 min

@Load 10.0 kg,
Temperature 250 °C
12.1 g/10 min

@Load 22.0 lb,
Temperature 482 °F
ASTM D1238
SABIC Innovative Plastics NORYL PX2622 PPE+HIPS (Asia Pacific)
PPE/HIPS for auto interior