Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 141R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 241 PC General Purpose polycarbonate with 10.5 of melt flow rate. Improved flame retardance. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 241R PC General purpose polycarbonate with 10.5 MFR and internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 241R PC (Asia Pacific) 10.5 MFR. Improved flame retardance. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 244R PC (Asia Pacific) LEXAN 244R resin grade is a medium viscosity multi purpose product with improved flame resistance and release properties. It is also FDA food contact compliant available in limited colors. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EX7631T PC EX7631T is a high UVA content homopolymer polycarbonate product intended for use as a cap layer for polycarbonate sheet extrusion. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HPS4 PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI).EtO, steam, e-beam, and gamma sterilizable... |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML6451 PC UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 141 PC General purpose polycarbonate with melt flow rate of 10.5. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® 141S PC (Asia Pacific) Nonhalogenated. 10.5 MFR. Internal mold release.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 143R PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 144R PC UL rated HB. 200 series recommended when V-2 rating required. MFR 10.5. Internal mold release. FDA food contact compliant in limited colors.Effective January 15th, 2007 this grade will no longer .. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 243 PC 10.5 MFR. UV-stabilized. Improved flame retardance. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 243R PC (Asia Pacific) 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman M2001-P Polyethylene
(discontinued **) M2001-P polyethylene is suggested for applications such as spiral-wound can linings, release paper and photographic paper. M2001-P has been found to exhibit good barrier properties, temperature res.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP4 PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mol.. |
|||
Melt Flow | 10.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® BC-0140 H ABS, Unreinforced General Purpose Stiff ABS material for automobile bobbinInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 10.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
10.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® SF-0505EH MABS, Unreinforced Scratch Resistant Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 10.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
10.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Asia Pacific) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Melt Flow | 10.5 g/10 min | 10.5 g/10 min | ASTM D1238 |
Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content Features: Recycled contentForm: PelletsInformation provided by Chase Plastics. |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake MC2001 High Density Polyethylene Coating Westlake MC2001 is a high density polyethylene designed for extrusion coating and lamination applications. MC2001 provides improved barrier properties, temperature resistance, stress crack resistanc.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® ET UV540 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• PC/UV absorber concent.. |
|||
Melt Flow | 10.5 g/10 min | 10.5 g/10 min | Condition S; ASTM D 1238 |
CPT C-Flex® R70-085 Clear Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
BASF Ultraform® N2320 0035 LEV POM Description: Is a POM, rapidly solidifying standard grade with improved impact strength for injection moldingInformation provided by BASF |
|||
Melt Flow | 10.5 g/10 min @Load 2.16 kg, Temperature 210 °C |
10.5 g/10 min @Load 4.76 lb, Temperature 410 °F |
|
Reliance Industries PVAXX H60 The key property of all PVAXX polymer is this product`s unique capacity to biodegrade into non-toxic residues under both aerobic and non-aerobic conditions.Information provided by Reliance Industrie.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 243R PC 10.5 MFR. UV-stabilized. Improved flame retardance. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP4NR PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 143R PC (Asia Pacific) Nonhalogenated. 10.5 MFR. UV-stabilized. Internal mold release. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |
|||
Melt Flow | 10.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® HP4NR PC (Europe-Africa-Middle East) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m.. |