Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Westlake MC2001 High Density Polyethylene Coating

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Westlake Chemical Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake MC2001 High Density Polyethylene Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Westlake MC2001 is a high density polyethylene designed for extrusion coating and lamination applications. MC2001 provides improved barrier properties, temperature resistance, stress crack resistance, scuff resistance, gloss and coefficient of friction (COF) compared to low density polyethylene.Application/UsesPhotographic paperRelease paperSpiral wound can liningsGrease barrierFDA: This material complies with FDA regulations in 21 CFR, section 177.1520.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D4883
Melt Flow 10.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
10.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 10 %
10 %
500mm/min; ASTM D638 Type IV Specimen
Flexural Modulus 0.965 GPa
140 ksi
Thermal Properties Metric English Comments
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Descriptive Properties Value Comments
Process Coating