Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
NOVA Chemicals Dylark® 232 High Performance Styrenic, Transparent Grade High heat resistance, Sparking water-white clarity, Good chemical resistance, High modulus, for superior shear and torque resistanceApplications: Light pipes and lighting, High heat microwave packag.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NOVA Chemicals Dylark® FG7300 High-Heat Styrenic Copolymer Product Description and Features: Styrene/maleic anhydride copolymer with high-heat resistance and high modulus. Resins designed for use in foam extrusion.Processing: Contact NOVA Chemicals techn.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Reliance Industries Repol R019MZ Polypropylene REPOL Polypropylene R019MZ is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | Condition G |
Ineos Nova 1230 High Heat Crystal Polystyrene
(discontinued **) Good processing characteristics, Low residual monomer, Low oligomersApplications: Direct injection foam, Biaxially oriented sheet, Glazing sheetExposure to gamma radiation in the 2.02-6.06 megarad r.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
BP Amoco Acctuf® 3119HS Ultra High Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Extrusion; ThermoformingFeatures: High stiffness, Low Temperature impactComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Samsung Cheil Industries Starex® HF-5330S ASA, Unreinforced
(discontinued **) Amorphous Styrene Acrylonitrile (SAN)Characteristics: Heat Resistant: Impact and Chemical Resistance, Surface GlossApplications: Oil Filter Case, Lubricant Can, Refrigerator and Hair Dryer Component.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills 43S2A Polypropylene Random Copolymer Features: Good clarity.Applications: Film extrusion and blow moldingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills P5G2K-096 Random Copolymer Polypropylene Features: Excellent clarity. Product does not contain animal derived components. Phthalate-freeApplications: Thermoforming, extrusion blow molding, injection blow molding, stretch blow molding, .. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills P5L2K-055 Polypropylene Random Copolymer Features: Excellent clarity. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding: extrusion blow molding, injection blow molding, stretch blow moldin.. |
|||
Melt Flow | 1.9 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.9 g/10 min @Load 11.0 lb, Temperature 392 °F |
Condition G; ASTM D1238 |
Global AS-320-PC Acrylonitrile Styrene, High Chemical/High Heat Resistance Grade Description-transparent, medium impact resistance, high hardness, good stiffness, high heat resistance, good chemical resistanceApplications-sanitary products, electrical partsInformation provided b.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos B4020N1331 Polyethylene Copolymer This is a unique high density polyethylene copolymer intended for the injection or compression molding of closures for beverages. Because of its high purity and excellent organoleptic properties, t.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos R01C-01 Polypropylene Random Copolymer This is a low flow rate, high clarity random copolymer designed for extrusion, thermoforming and blow molding. Applications that require good see-through clarity combined with good heat resistance .. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ISO 1133 |
Iran Petrochemical (PCC) 2602TH00 Low Density Polyethylene LDPE 2602TH00 high clarity film Applications: film, underblankets and films for medical applications.Information provided by Iran Petrochemical Commercial Co. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE3-0202ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing antimicrobial protection.All information provided by LTL Color Compounders, Inc. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LTL Color Compounds ColorRxâ„¢ PE3-0205ARX Biocompatible, Antimicrobial LDPE A biocompatible Low Density Polyethylene for healthcare applications containing a high level of antimicrobial protection for FDA regulated medical devices.All information provided by LTL Color Compo.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ISO 1133 |
Lucite International Diakon® TD525 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Melt Flow | 1.9 g/10 min | 1.9 g/10 min | ASTM D1238 |
Flint Hills P5M2Z-012 Polypropylene Random Copolymer Features: Good contact clarity. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: film and blow moldingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Iran Petrochemical (PCC) LF0190 Low Density Polyethylene LF01090 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: general pupose film and for aminati.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Borealis Bormed™ RB845MO Random Copolymer for Healthcare Applications Bormed RB845MO is a random copolymer for blow molding with very good transparency and high contact clarity, very good gloss and surface finish. Bottles in sizes up to 2 quarts molded from Bormed RB.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont 20 Series 20-6064 Specialty Polyethylene Resin DuPont 20-6064 specialty low density polyethylene resin is characterized by low melt index and intermediate crystallinity. This product, produced via a unique polymerization process, has outstanding.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA offers good toughness and optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: NoApplications: Coextrus.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 380BA Wire & Cable Low Density Polyethylene Resin (European Grade) Product Description: LD 380BA is a non-stabilized LDPE, designed for the production of Low Voltage power cable insulation using the two-step silane cross-linking technology. Sufficient antioxidant a.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow INSPIRE™ D560.00 Developmental Performance Polymer D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended f.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg |
1.9 g/10 min @Load 4.76 lb |
|
Dow LDPE 501I Low Density Polyethylene, Clear Film Grade DOW LDPE 501I, a barefoot resin used for bakery film and other packaging applications that require optical clarity. This material complies with U.S.FDA regulation 21 CFR 177.1520(c) 2.1 for food con.. |
|||
Melt Flow | 1.9 g/10 min @Temperature 230 °C |
1.9 g/10 min @Temperature 446 °F |
ASTM D1238 |
Dow 6D83K Polypropylene Resin DOW 6D83K is intended for use in extrusion blow molding processes where enhanced clarity is desired.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July .. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem PB 682 LDPE Blow Molding Polyethylene Description: PB682 is a low density polyethylene (LDPE), produced under high pressure technology. The end products molded with this resin present good dimensional stability and high flexibility.Appl.. |
|||
Melt Flow | 1.9 g/10 min @Load 2.16 kg, Temperature 235 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 455 °F |
|
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Dry) Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t.. |
|||
Melt Flow | 1.9 g/10 min @Load 1.90 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.19 lb, Temperature 446 °F |
ISO 1133 |
Borealis RB206MO-06 Polypropylene Random Copolymer RB206MO-06 is a random copolymer with good transparency and contact clarity, very good gloss and surface finish. The high stiffness of this grade allows for a reduction in cycle time. This grade als.. |