Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Plastcom SLOVAMID 6 GF 65/1M PA6 reinforced with 65% glass fibre Features: PA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |
|||
Melt Flow | 1.0 g/10 min @Load 0.325 kg, Temperature 270 °C |
1.0 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVAMID 66 GF 15 GB 25 TS PA66, 15% glass fibre, 25% glass beads FeaturesPA 66 chemically reinforced with 15 % glass fibre and with the content of 25% glass beads, thermo stable. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical p.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVAMID 66 GF 25 FRG 5 Polyamide 66, 25% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 66 for injection moulding, chemical reinforced with 25% glass fiber and non-halogen flame retardant, with heat and flammability resistance, achieves V-0 in accordance with UL 94. Non-hal.. |
|||
Melt Flow | 1.0 g/10 min @Load 0.325 kg, Temperature 270 °C |
1.0 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVAMID 66 GF 25 FRI 2 PA66, 25% glass fibre, flame retardant FeaturesPA 66 for injection moulding, chemically reinforced with 25% glass fibre and non-halogen flame retardant, with heat resistance and nonflammability, achieves V 0 in accordance with UL 94. Non.. |
|||
Melt Flow | 1.0 - 5.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 5.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Polymer Resources AC-GP1 Acetal Copolymer, Low Flow, High Melt Strength Process: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 1.0 - 3.0 g/10 min @Load 11.6 kg, Temperature 250 °C |
1.0 - 3.0 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-FR6 Modified-PPO, V-0 Flame Retardant Modified-Polyphenylene Oxide, V-0 Flame Retardant, 300F HDTFeatures: • Bromine Free • Chlorine FreeProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVAMID 6 GF 50 Polyamide 6, 50% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 50% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Melt Flow | 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G2706-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G2706-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA and medical compliance. - High Puncture Reseal - Overmold Adhesion to Po.. |
|||
Melt Flow | 1.0 g/10 min | 1.0 g/10 min | Condition E; ASTM D 1238 |
Eastman 5222 LDPE 6% VA Copolymer, High Clarity, Ultra-High Impact Film Resin
(discontinued **) Resin Type: VA CopolymerCharacteristics: Excellent impact strength, Good low temperature properties, Good heat seal characteristics, High slip, High antiblock, Good optical propertiesApplications:Ic.. |
|||
Melt Flow | <= 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
<= 1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D1101 A (SBS) Liner Block Copolymer Description: Kraton D1101 A polymer is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 31% mass. It is supplied from Europe in the physical forms identified as f.. |
|||
Melt Flow | <= 1.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
<= 1.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D1101 B (SBS) Liner Block Copolymer Description: Kraton D1101 B is a clear, linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from South America in the physical form(s) identifi.. |
|||
Melt Flow | 1.0 g/10 min | 1.0 g/10 min | ISO 1133 |
Lucite International Diakon® CMH454L Acrylic Polymer Information provided by Lucite International |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Hostacomâ„¢ BA742EC Polypropylene Copolymer Description: Hostacomâ„¢ BA742EC low melt flow, 1,200 MPa flexural modulus, precolored, extrusion grade polypropylene copolymer has a good balance of strength, stiffness, impact resistance and pr.. |
|||
Melt Flow | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Westlake Hifor LT74105 Linear Low Density Polyethylene WESTLAKE Hifor Polyethylene LT74105 is a high strength linear low density polyethylene containing medium slip and medium antiblock. It is designed for blown film applications and is well suited for.. |
|||
Melt Flow | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Westlake Hifor Xtreme SC74838 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74838 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains medium slip and medium antiblock. Films produced with this re.. |
|||
Melt Flow | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Melt Flow | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYFLAM™ RABS 930-01 Information provided by A. Schulman. |
|||
Melt Flow | 1.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D 1238 |
Cossa Polimeri ESTAPROP H0260 MC/EC Conductive Polypropylene, Mineral Filled Information provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ELASTO UK Dryflex® 502450S SEBS Based Material, Unfilled Qualities, 45A Hardness, Black The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LL 1001x72 Blown Film Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 1001X26 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 1001X74 Linear Low Density Polyethylene Resin Product Description: LL 1001 are butane LLDPE blown film resins having good draw down. Films made from LL 1001 resins exhibit good tensile and toughness properties. Availability: Latin America, Nort.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LLDPE LL 3001.32 Cast Linear Low Density Polyethylene Resin Product Description: LL 3001.32 is a hexane copolymer LLDPE designed for the blown or cast film process. Films made from LL 3001.32 have outstanding tensile and toughness properties. The superior st.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg |
1.0 g/10 min @Load 4.76 lb |
ASTM D1238 |
Equate EFDC-7087 LLDPE Film Extrusion Resin EFDC-7087 is a linear low-density polyethylene resin for tubular blown film extrusion. Films made from EFDC-7087 have good toughness, high tensile strength and outstanding puncture resistance. EFDC-.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg |
1.0 g/10 min @Load 4.76 lb |
|
Dow LDPE 527A Low Density Polyethylene, Blown Film Grade DOW LDPE 527A is a general purpose blown film extrusion resin for use in medium duty liner film applications and other packaging applications. It contains high levels of antiblock additive. This mat.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem LL118/21 Blown Film Extrusion Linear Low Density Polyethylene Description: LL118/21 is a LLDPE Butene copolymer produced by Braskem. It is a general purpose product that shows a good processing performance balanced with good optical and mechanical properties a.. |
|||
Melt Flow | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Carmel Olefins IPETHENE® 213 Low Density Polyethylene IPETHENE® 213 is a general purpose low density polyethylene film extrusion grade. It contains a medium level of anti-blocking and slip additives. It is BHT free. It exhibits a good balance between .. |
|||
Melt Flow | 1.0 g/10 min | 1.0 g/10 min | ISO 1133 |
Ashley Polymers Ashlene® RH180ST Acetal A high impact homopolymer resin.Data provided by the manufacturer |
|||
Melt Flow | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
ExxonMobil LL 1001x59 Blown Film Resin
(discontinued **) LL1001 are butene LLDPE blown film resins having good drawdown, tensile and toughness properties.Information provided by ExxonMobil Chemical |