Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FC 20 Low Density Polyethylene - Blown Film Extrusion Riblene FC 20 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 20 is characterized by a high melt strength leading to a good bubble sta.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FC 26 Low Density Polyethylene - Blown Film Extrusion Riblene FC 26 is a high molecular weight low density polyethylene (LDPE), with added antiblocking agent, suitable for blown film extrusion. Riblene FC 26 is characterized by a high melt strength le.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polimeri Europa Riblene® FC 39 Low Density Polyethylene - Blown Film Extrusion Riblene FC 39 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FC 39 is characterized by a high melt strength leading to a good bubble stability.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® LF-Y320-D Fractional Melt LDPE Film Resin Features: High melt strength and superior bubble stabilityEnhances throughputs in LLDPE blendsSuperior strength and toughnessExcellent shrink film characteristics Applications: Industrial packagingL.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
ExxonMobil LD 051.LJ Molding, Extrusion and Compounding Resin
(discontinued **) LD 051.LJ resin is used in Blow molded, squeeze bottles, Pail lids, Closures, and Extruded profiles.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ExxonMobil Method |
ExxonMobil LD 641.LN Molding, Extrusion and Compounding Resin
(discontinued **) LD 641.LN is a low density homopolymer specifically designed for high performance blow molding applications. This resin is suitable for applications requiring high melt strength, flexibility, good .. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D 1238 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem PB 526 LDPE Blow Molding Polyethylene
(discontinued **) Applications: Heavy duty bags; tubes and hoses; shrink films for pallets; tarpaulins. Blown Film. Information provided by Braskem |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ineos G60-25-144 HDPE Ineos G60-25-144 is a high density polyethylene homopolymer typically used in the production of sheet extrusion and blow molded containers. This material meets the Food and Drug Administration requ.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUTENE-H BE0400 HDPE Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical LUTENE-H PE0235 HDPE Description: LUTENE-H PE0235 is a materials with high toughness and rigidity suitable for cable protection It has very high resistance to stress cracking and long-term internal pressure creep proper.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA480177 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA480178 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Blow Molding) ApplicationsPETROTHENE NA 940-000 is a low density homopolymer resin intended for use in blow molding applications. Excellent toughness, good clarity and processability make NA 940-000 an ideal cho.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Lucobit Lucofin® 1400HN Powder Ethylene Butyl Acrylate Lucofin 1400HN Powder is a polar copolymer consisting of ethylene and butyl acrylate with low crystallinity. Due to its chemical structure Lucofin 1400HN Powder is softer and more flexible than ethy.. |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
SCG Chemicals EL-Leneâ„¢ H1000PC High Density Polyethylene Pipe Resin Key Characteristics: Good processing, high thermal stability, low sagging, good balance of MRS, SCG, and RCPRecommended Applications: Water pressure and gas pipesCertification: Certified by EXOVA.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis BorECO™ BA222E Polypropylene Block Copolymer for Non-Pressure Pipes BorECO BA222E is a high molecular weight, low melt flow rate polypropylene block copolymer with superior stiffness and excellent impact properties. BorECO BA222E fulfills the requirements according.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis Casico™ FR6082 Reduced Fire Hazard Jacketing Compound Casico™ FR6082 is a thermoplastic, reduced fire hazard, zero halogen black jacketing compound combined with high mechanical strength, toughness and excellent extrusion properties. It is based on th.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RA130E Polypropylene Random Copolymer RA130E is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is natural colored. Applications RA130E is recommended for the production of PP-R pipes and .. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RA130E-1498 Polypropylene Random Copolymer RA130E-1498 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is white colored. Applications: RA130E-1498 is recommended for the production of PP-R p.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
Formosa Plastics Formolene® HB5502S1 Sheet and Thermoforming HDPE High Density Polyethylene Hexene CopolymerApplications: Molded or formed industrial housings and parts, tanks, shrouds.Formolene HB5502S1 HDPE resin is designed for applications requiring excellent .. |
|||
Melt Flow | 0.25 g/10 min @Load 5.00 kg, Temperature 190 °C |
0.25 g/10 min @Load 11.0 lb, Temperature 374 °F |
ISO 1133 |
Borealis BorSafe™ HE3490-LS-H HDPE Compound for Pressure Pipes BorSafe™ HE3490-LS-H is a bimodal polyethylene compound produced by the advanced Borstar® technology. It includes a combination of pigments and stabilizers to ensure excellent long-term thermal s.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis RA130E-8427 Polypropylene Random Copolymer RA130E-8427 is a high molecular weight, low melt flow rate polypropylene random copolymer (PP-R) compound and is grey colored. Applications: domestic water, heating, relining, plumbing, and industr.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.25 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ FL 00014 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00014 is a copolymer of ethylene and vinyl acetate. For film requiring very high toughness, low creep, excellent optical properties and low gel.Availability: Africa & Middle .. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ExxonMobil Method |
ExxonMobil LD 317.09 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ExxonMobil Method |
ExxonMobil LD 317.87 Film Resin LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon.. |
|||
Melt Flow | 0.25 g/10 min @Load 2.16 kg |
0.25 g/10 min @Load 4.76 lb |
ASTM D 1238 |
Total Finathene® RS 528 HDPE blow molding
(discontinued **) Applications: Bleach and detergents, industrial chemicals, industrial parts, cosmetic bottles, food packaging.Information provided provided by Total Petrochemicals.Total Petrochemicals includes form.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | ASTM D1238 |
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Film Grade) ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for.. |
|||
Melt Flow | 0.25 g/10 min | 0.25 g/10 min | Condition 190/2.16; ASTM D1238 |
Chevron Phillips Marlex® HHM 5502-01 ST High Density Ethylene Hexene Copolymer High Density Ethylene Hexene CopolymerSag Upper Limit: 18 cm, Lower Limit: 13 cm; 2 ft. X 4ft. X 125 mil thick blank heated to forming temperature.Data provided by Chevron Phillips Chemical Company.. |