Polymer Property : Apparent Bulk Density = 0.0325 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.750 - 0.900 g/cc
0.0271 - 0.0325 lb/in³
ISO 60
Raschig Group 5553 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Apparent Bulk Density 0.750 - 0.900 g/cc
0.0271 - 0.0325 lb/in³
ISO 60
Raschig Group 5562 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Apparent Bulk Density 0.750 - 0.900 g/cc
0.0271 - 0.0325 lb/in³
ISO 60
Raschig Group 5563 DAP
Glass-fiber reinforced diallyl phthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensiona..
Apparent Bulk Density 0.700 - 0.900 g/cc
0.0253 - 0.0325 lb/in³
ISO 60
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..
Apparent Bulk Density 0.700 - 0.900 g/cc
0.0253 - 0.0325 lb/in³
ISO 60
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Apparent Bulk Density 0.700 - 0.900 g/cc
0.0253 - 0.0325 lb/in³
ISO 60
Raschig Group AMPLA® 7500 melamine-modified polyester
Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta..
Apparent Bulk Density 0.700 - 0.900 g/cc
0.0253 - 0.0325 lb/in³
ISO 60
Raschig Group DECAL® 572R Phenolic
Glass-fiber reinforced phenolic molding compound. Exceptional heat resistance with regard to maintaining surface finish and mechanical properties, outstanding mechanical properties, excellent rotati..
Apparent Bulk Density 0.700 - 0.900 g/cc
0.0253 - 0.0325 lb/in³
ISO 60
Raschig Group DECAL® 666/8 Phenolic
Glass-fiber reinforced phenolic molding compound with mineral fillers. High heat resistance, reduced mould shrinkage and post-shrinkage, good chemical resistance and mechanical properties. This prod..
Apparent Bulk Density 0.700 - 0.900 g/cc
0.0253 - 0.0325 lb/in³
ISO 60
Raschig Group DECAL® 937 Phenolic
Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W..
Apparent Bulk Density 0.600 - 0.900 g/cc
0.0217 - 0.0325 lb/in³
ISO 60
Raschig Group EPOXIDUR® 3580 EP Epoxy
Glass-fiber reinforced and mineral filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties even with thin wall thicknesses and high temperatures. This prod..
Apparent Bulk Density 0.270 - 0.900 g/cc
0.00975 - 0.0325 lb/in³
Average value: 0.684 g/cc Grade Count:29
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor..
Apparent Bulk Density 0.750 - 0.900 g/cc
0.0271 - 0.0325 lb/in³
ISO 60
Raschig Group 5567 DAP Diallyl Phthalate (DAP), Cast, Mineral Filler
Glass-fiber reinforced diallyl phthalate molding compound free from halogens. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exc..
Apparent Bulk Density 0.750 - 0.900 g/cc
0.0271 - 0.0325 lb/in³
ISO 60
Raschig Group 5557 DAP  (discontinued **)
Glass fiber-reinforced and inorganically filled diallylphthalate molding compound (DAP) in various colors. Good mechanical strength together with retention of high electrical properties under hot h..