Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 10000 - 20000 cP @Temperature 25.0 °C |
10000 - 20000 cP @Temperature 77.0 °F |
Uncured |
Permabond TA459 Toughened Acrylic Adhesive Permabond TA459 is a structural acrylic adhesive designed primarily for bonding metals, ferrites, ceramics and some thermoplastics. This product was specifically designed to be non-corrosive to sens.. |
|||
Viscosity | 16000 - 20000 cP | 16000 - 20000 cP | |
Huntsman Araldite GY 6020 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 185 to 200. Max color is 1.Comments/Applications: Higher viscosity GY 6010, unmodified. General purpose higher viscosity resin.Data provided by Ciba Specialty Chemic.. |
|||
Viscosity | 7000 - 20000 cP | 7000 - 20000 cP | |
Huntsman Araldite PZ 3901 Water-Based Adhesive/Coating Base Resin is GT 7071 (Type 1). Typical Solids Content 55%. Mean Particle Size |
|||
Viscosity | 7000 - 20000 cP | 7000 - 20000 cP | |
Huntsman Araldite PZ 3902 Water-Based Adhesive/Coating Typical Solids Content 53%. Mean Particle Size |
|||
Viscosity | 8000 - 20000 cP | 8000 - 20000 cP | |
Huntsman Araldite PZ 3907 Water-Based Adhesive/Coating Base Resin is GT 7097 (Type 7). Typical Solids Content 55%. Mean Particle Size |
|||
Viscosity | 8000 - 20000 cP | 8000 - 20000 cP | |
Huntsman Araldite XU 3903 Water-Based Adhesive/Coating Base Resin is GT 7013 (Type 3). Mean Particle Size |
|||
Viscosity | 10000 - 20000 cP | 10000 - 20000 cP | |
Huntsman Araldite XU 3917 Water-Based Adhesive/Coating Base Resin is GT 7097 (Type 7). Typical Solids Content 55%. Mean Particle Size |
|||
Viscosity | 10000 - 20000 cP | 10000 - 20000 cP | B |
ITW Plexus Plexusâ„¢ MA422 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, medium open time.Information provided by Illinois Tool Works. |
|||
Viscosity | 10000 - 20000 cP | 10000 - 20000 cP | B |
ITW Plexus Plexusâ„¢ MA555 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low exotherm adhesive able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Viscosity | 10000 - 20000 cP | 10000 - 20000 cP | Part B |
Master Bond EP37-3FLFAN Electrically Isolating, Flexible Epoxy Description: Master Bond Polymer System EP37-3FLFAN is a two component system for high performance potting, bonding, sealing and coating that is formulated to cure at room temperature or more rapidl.. |
|||
Viscosity | 12000 - 20000 cP | 12000 - 20000 cP | Mixed system |
Master Bond Ep46HT-2 Two Component, Heat Resistant Epoxy System Master Bond Polymer System EP46HT-2 is a two component epoxy system for bonding, sealing and casting applications where resistance to temperatures from -100°F to +500°F is required. It is 100% rea.. |
|||
Viscosity | 12000 - 20000 cP @Temperature 23.0 °C |
12000 - 20000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® 353ND-T1 High Temperature Thixotropic Epoxy Material Description: A two component, thixotropic and high temperature epoxy designed for fiber optic, electronics and medical applications. It is a more viscous alternative to EPO-TEK® 353ND-T.I.. |
|||
Viscosity | 10000 - 20000 cP @Temperature 23.0 °C |
10000 - 20000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® E2036 Epoxy Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o.. |
|||
Viscosity | 10000 - 20000 cP @Temperature 23.0 °C |
10000 - 20000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® H20E-8 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H20E-8 is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is a higher viscos.. |
|||
Viscosity | 12000 - 20000 cP @Temperature 23.0 °C |
12000 - 20000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® H22 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® H22 is a two component, silver-filled epoxy system designed specifically for die bonding and sealing hybrid circuit packages.Advantages & Application Notes: A smooth, .. |
|||
Viscosity | 5000 - 20000 cP | 5000 - 20000 cP | |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 14000 - 20000 cP | 14000 - 20000 cP | 50-1 |
Abatron AboCast 50-3/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin.. |
|||
Viscosity | 10000 - 20000 cP | 10000 - 20000 cP | |
Aremco Pyro-Paint™ 634-AS1 High Temperature Refractory Coating This alumina-silica based advanced coating is rated for continuous service temperatures up to 2300 °F. Provides excellent adhesion to ceramic fiber blankets, modules and boards and resists wetting .. |
|||
Viscosity | 14000 - 20000 cP | 14000 - 20000 cP | 50-1 |
Abatron AboCast 50-6/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months. |
|||
Viscosity | 15000 - 20000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
15000 - 20000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK2.1° |
Gwent Electronic Materials D2090124D2 Green Solder mask Dielectric This product has been designed as a solder mask dielectric for use at high temperatures. It has been tested at 250°C and was proved to be stable for 12 weeks. Screen Printing Equipment: semi-automa.. |
|||
Viscosity | 10000 - 20000 cP | 10000 - 20000 cP | B |
ITW Plexus Plexus™ MA922 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, medium open time.Information provided by Illinois Tool Works. |
|||
Viscosity | 10000 - 20000 cP | 10000 - 20000 cP | B |
ITW Plexus Plexus™ MA925 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works. |
|||
Viscosity | 8000 - 20000 cP | 8000 - 20000 cP | |
Beijing Ranger Chem SM-602RX70 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |