Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 12000 - 16000 cP | 12000 - 16000 cP | |
ND Industries 440 High pressure Sealant Pneumatic and hydraulic sealant fluid, for power and gas system connections |
|||
Viscosity | 10000 - 16000 cP | 10000 - 16000 cP | Of hardener at 25C |
Resin Technology Group TIGA 101-EX Five-Minute Epoxy Adhesive 1 part resin to 1 part hardener.TIGA 101-EX is an exceptional epoxy formulation, recommended for lower temperature or wet industrial bonding applications where fast curing is required. This clear, t.. |
|||
Viscosity | 8000 - 16000 cP @Temperature 175 °C |
8000 - 16000 cP @Temperature 347 °F |
Automatic orifice Viscosity |
Cookson Group Plaskon® 3400 Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A reduced-stress epoxy molding compound for the encapsulation of a variety of semiconductor devices ranging from small lead count.. |
|||
Viscosity | 6000 - 16000 cP | 6000 - 16000 cP | |
Huntsman AroCy XU 71787.07 L Cyanate Ester Comments/Applications: Toughened Dicyclopentadiene based cyanate ester resin.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman. |
|||
Viscosity | 14000 - 16000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
14000 - 16000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2050303D1 Fine Line Printing Ink Silver Ink has been designed for fine line printing. It is capable of printing down to 50 micron line and spaces within a production environment. Under laboratory conditions, finer lines and spaces .. |
|||
Viscosity | 11000 - 16000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
11000 - 16000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2061103D7 Lead free Silver Zinc Basecoat Paste This product is a lead-free version of C70709D22. The ink is designed as a screen printing ink for coating Barium Titanate PTC ceramics as the base layer of a two part system. The dried film should.. |
|||
Viscosity | 14000 - 16000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
14000 - 16000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2070423D5 Polymer Dielectric Grey colored screen printable polymer dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode. The formulation i.. |
|||
Viscosity | 12000 - 16000 cP @Temperature 23.0 °C |
12000 - 16000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® OE120 Two Component Epoxy Material Description: A two component, opaque epoxy, designed for fiber optics packaging applications. It is a black-colored version of EPO-TEK 353ND-T. It has a high Tg for resisting elevated ope.. |
|||
Viscosity | 12000 - 16000 cP | 12000 - 16000 cP | uncured |
Atom Adhesives AA-BOND FDA2 Epoxy Adhesive AA-BOND FDA2 is a medium viscosity epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and recei.. |
|||
Viscosity | 7000 - 16000 cP | 7000 - 16000 cP | Base |
3M Scotch-Weld™ DP270 Black Structural Adhesive Rigid potting compound, Non-corrosiveInformation provided by 3M |