Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 11000 - 14000 cP | 11000 - 14000 cP | |
Huntsman Araldite GY 6010 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 182 to 192. Max color is 1.Comments/Applications: Unmodified basic liquid epoxy resin based on bis A and epichlorohydrin. General purpose, highly versatile resin for.. |
|||
Viscosity | 11000 - 14000 cP | 11000 - 14000 cP | |
Huntsman Quatrex 1010 Bisphenol A Epoxy Resin Weight per Epoxide (EEW, g/eq) 182 to 190.Comments/Applications: High purity bisphenol-A based epoxy resin.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Hun.. |
|||
Viscosity | 10500 - 14000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
10500 - 14000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2030217D2 Aluminium for PTC paste Aluminium Ink designed to give good ohmic contact on to barium titanate PTC components. This product is particularly good where large volumes of PTC components are being processed in belt furnaces .. |
|||
Viscosity | 9500 - 14000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
9500 - 14000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2080121D12 Dielectric Ink This product is a thermoplastic screen printing ink, developed for use for flexible polymer applications. It is printed on to flexible polymeric substrates, such as Polyimide and PET substrates, to .. |
|||
Viscosity | 9000 - 14000 cP @Temperature 40.0 °C |
9000 - 14000 cP @Temperature 104 °F |
|
Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | Part A |
Master Bond EP21LV-LO Two Component, Lower Viscosity, Room Temperature Curing Epoxy System Product Description: Master Bond EP21LV-LO is a two component, lower viscosity, room temperature curing epoxy system for high performance bonding, sealing, coating and encapsulation. This user frien.. |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | Part A |
Master Bond EP21LVMed Two Component, Low Viscosity USP Class VI Epoxy Master Bond EP21LVMed is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulating and casting. It is formulated to cure readily at room tempera.. |
|||
Viscosity | 9000 - 14000 cP | 9000 - 14000 cP | Part A |
Master Bond EP21TDC-4 Two Component, Highly Flexible Epoxy System Master Bond Polymer System EP21TDC-4 is a two component, flexible epoxy resin system for high performance bonding, sealing and coating. It is formulated to cure at ambient temperatures or more quick.. |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | Part A |
Master Bond EP30-3LO Highly versatile, two part epoxy system for bonding, coating, sealing and casting Master Bond EP30-3LO is a two component epoxy system featuring a combination of optical clarity and light transmission, good glass transition temperature (Tg), great chemical resistance along with p.. |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | Part A |
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | Part A |
Master Bond EP21CLV Two Component Epoxy System Product Description: Master Bond EP21CLV is a two component, lower viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It features easy handling a.. |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | Part A |
Master Bond EP41SMed Two Component, Low Viscosity, USP Class VI Epoxy System Master Bond Polymer Adhesive EP41S Medical is a two component low viscosity epoxy resin system for high performance bonding, sealing, coating, as well as small encapsulations, pottings and castings... |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | Part A |
Master Bond EP42-2LV Epoxy Resists Heat and Chemicals Description: Master Bond Polymer System EP42-2LV is a low viscosity room temperature curable two component epoxy, adhesive, sealant, coating and casting material featuring outstanding chemical resis.. |
|||
Viscosity | 10000 - 14000 cP @Temperature 23.0 °C |
10000 - 14000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® 730 Unfilled Black General and Structural Grade Epoxy Material Description: A two component, room temperature curing, general and structural grade epoxy. It can be used for adhesive, sealing, and encapsulating applications in medical, xray device, fil.. |
|||
Viscosity | 11000 - 14000 cP @Temperature 23.0 °C |
11000 - 14000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® E2001-HV Electrically Conductive, Silver-Filled Epoxy Product Description: EPO-TEK® E2001-HV Is a snap cure, two component, silver-filled die attach adhesive for semiconductor plastic IC packaging.Advantages & Application Notes:Snap cure adhesive or f.. |
|||
Viscosity | 11000 - 14000 cP @Temperature 23.0 °C |
11000 - 14000 cP @Temperature 73.4 °F |
20 rpm |
Epoxy Technology EPO-TEK® E3001-HV Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E3001-HV is a snap cure, single component, silver-filled die attach adhesive for semiconductor plastic IC packaging. Also available in a frozen syringe. Advantages & .. |
|||
Viscosity | 8000 - 14000 cP | 8000 - 14000 cP | Accelerator |
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Viscosity | 8000 - 14000 cP | 8000 - 14000 cP | Accelerator |
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat.. |
|||
Viscosity | 6000 - 14000 cP | 6000 - 14000 cP | |
Beijing Ranger Chem 0164P Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 8000 - 14000 cP | 8000 - 14000 cP | |
Beijing Ranger Chem 164 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 12000 - 14000 cP | 12000 - 14000 cP | |
Aremco Aremco-Seal™ 529VHV High Temperature Specialty Coatings Silicone Very high viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |
|||
Viscosity | 11000 - 14000 cP | 11000 - 14000 cP | 50-3 |
Abatron AboCast 50-3/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Honey viscosity, light amber color. Best combination of high strength and versatility for Abatron "VR" Epoxies. Shelf life is 12+ months.Processin.. |
|||
Viscosity | 11000 - 14000 cP | 11000 - 14000 cP | 50-3 |
Abatron AboCast 50-3/AboCure 50-12 Epoxy Data provided by the manufacturer, Abatron, Inc. Light motor oil viscosity, almost colorless. Shelf life is 12+ months. |
|||
Viscosity | 8000 - 14000 cP | 8000 - 14000 cP | Accelerator |
3M Scotch-Weld™ DP420 LH Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Viscosity | 8000 - 14000 cP | 8000 - 14000 cP | Accelerator |
3M Scotch-Weld™ DP420 NS Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M |
|||
Viscosity | 11000 - 14000 cP | 11000 - 14000 cP | Dynamic |
Dow Corning 3-0135 Cosmetic Fluid Polydimethylsiloxane polymer with terminated, curable silanol functionality.Information provided by Dow Corning |
|||
Viscosity | 8000 - 14000 cP | 8000 - 14000 cP | Accelerator |
3M Scotch-Weld™ DP405 Black Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP405 LH is a two-part, 2:1 mix ratio, toughened epoxy structural adhesive which has a 5 minute work life and accelerated cure. It exhibits excellent shear and peel.. |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | |
Beijing Ranger Chem HY-128 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 11000 - 14000 cP | 11000 - 14000 cP | 50-3 |
Abatron AboCast 50-3/AboCure 50-17 Epoxy Data provided by the manufacturer, Abatron, Inc. Very low-viscosity; Dark Amber color. Shelf life is 12+ months. |
|||
Viscosity | 10000 - 14000 cP | 10000 - 14000 cP | Part A |
Master Bond EP30M4LV Chemically Resistant, Low Viscosity Adhesive Description: Master Bond EP30M4LV is a two component, low viscosity epoxy system for high performance bonding, sealing and encapsulation. This system features a forgiving 100 to 60 mix ratio by weig.. |