Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 400 - 1000 cP @Temperature 25.0 °C |
400 - 1000 cP @Temperature 77.0 °F |
|
Northstar Polymers PCA-054 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1000 cP @Temperature 25.0 °C |
800 - 1000 cP @Temperature 77.0 °F |
Uncured |
Permabond UV610 UV-curable Adhesive PERMABOND UV610 is a single part, fast setting, UV curable adhesive designed specifically for bonding glass and metal. Its high strength makes it suitable for a wide range of applications including .. |
|||
Viscosity | 800 - 1000 cP @Temperature 23.9 °C |
800 - 1000 cP @Temperature 75.0 °F |
|
TSE Industries EcoWIND® 100 Polyurethane Resin Filament Winding
(discontinued **) TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Viscosity | 400 - 1000 cP | 400 - 1000 cP | |
Huntsman AroCy XU 366 Cyanate Ester Comments/Applications: Lowest cure temperature (250°F) cyanate ester. Exceptional dielectric properties. Uses include microwave antennas, radomes, structural and electronic grade adhesives.Data.. |
|||
Viscosity | 600 - 1000 cP | 600 - 1000 cP | |
Huntsman AroCy XU 378 Cyanate Ester Comments/Applications: Novolac cyanate ester. High temperature composites and adhesives, where a Tg greater than 300°C is required.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemic.. |
|||
Viscosity | 600 - 1000 cP | 600 - 1000 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1114 P (SIS) Linear Triblock Copolymer Description: Kraton D1114 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 19%. It is supplied from North America in the physical form identified: .. |
|||
Viscosity | 500 - 1000 cP | 500 - 1000 cP | ASTM D803 |
SK Chemicals SKYTHANE® US106B Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 350 - 1000 cP | 350 - 1000 cP | RPG30 |
Solvay ALKAMULS® EL 620 LI E Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Identification: CASTOR OIL ETHOXYLATE (30)CAS: 61791 – 12 â€.. |
|||
Viscosity | 250 - 1000 cP | 250 - 1000 cP | |
Solvay ALKAMULS® EL 620 Surfactant Description: Castor oil ethoxylate (30 EO) Emulsifier for fats, oils fatty acids and solvents. Maintains stability of oil-in-water emulsions over a wide temperature range as co-emulsifier with an HL.. |
|||
Viscosity | 350 - 1000 cP | 350 - 1000 cP | #3 SP @ 60 RPM; RP-0659 |
Solvay ALKAMULS® EL 620LI Surfactant Description: Biodegradable castor oil ethoxylate emulsifier, solubiliser for a wide range of formulations with an HLB of around 12.Chemical Name: CASTOR OIL ETHOXYLATE(30)CAS: 61791-12-6, 7732-18-5A.. |
|||
Viscosity | 600 - 1000 cP | 600 - 1000 cP | #3 sp @ 60 rpm; RP-0596 |
Solvay RHODOLINE® LC-2 Surfactant Description: Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: DEFOAMER BLENDAvailable in: North America.. |
|||
Viscosity | 500 - 1000 cP @Temperature 82.2 °C |
500 - 1000 cP @Temperature 180 °F |
|
Master Bond EP36CLV One Component Heat Resistant Liquid Flexible Epoxy Master Bond Polymer System EP36CLV is a one component, high temperature resistant, B staged epoxy that cures with excellent toughness and is far less rigid than typical high temperature resistant ep.. |
|||
Viscosity | 800 - 1000 cP | 800 - 1000 cP | Part A |
Master Bond EP45HT-1 Adhesive Resists Exposure to Sterilization Description: Master Bond Polymer System EP45HT-1 is a remarkably fast curing, medium viscosity, two component epoxy compound formulated for high performance casting and bonding. It is 100% reactive .. |
|||
Viscosity | 100 - 1000 cP | 100 - 1000 cP | Part B |
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Viscosity | 200 - 1000 cP | 200 - 1000 cP | Part B |
Master Bond EP42HT-2AO-1 Two Part, Cryogenically Serviceable Epoxy Description: Master Bond EP42HT-2AO-1 Black is a room temperature curable, two component epoxy adhesive, sealant, coating and casting material that meets NASA low outgassing specifications. It featu.. |
|||
Viscosity | 700 - 1000 cP | 700 - 1000 cP | NOV QC 020 |
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 500 - 1000 cP @Temperature 23.0 °C |
500 - 1000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 337H Graphite-Filled, High Temperature Epoxy Product Description: EPO-TEK® 377H is a two component, high Tg, graphite filled epoxy designed for ESD/EMI shielding of semiconductor devices and electronics. It can be used in many electronic ind.. |
|||
Viscosity | 400 - 1000 cP @Temperature 23.0 °C |
400 - 1000 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 509FM-1 General Purpose Epoxy Product Description: EPO-TEK® 509FM-1 is a two component, optically opaque epoxy designed for potting of semiconductors, PCB and systems-level electronics. It can be used in many electronic indust.. |
|||
Viscosity | 500 - 1000 cP | 500 - 1000 cP | |
Beijing Ranger Chem SM-828X90 Solvent Based Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 500 - 1000 cP | 500 - 1000 cP | |
Aremco Ceramacoat™ 845-BLU High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, blue coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, stadiu.. |
|||
Viscosity | 800 - 1000 cP | 800 - 1000 cP | |
Aremco Ceramacoat™ 845-GDK High Temperature Ceramic-Inorganic Coating Single part, waterborne, silicon-filled, phosphate-bonded, dark green coating for glass and quartz to 2000 ºF (1093 ºC). Primarily used for marking ceramic parts and coating automotive headlamps, .. |
|||
Viscosity | 800 - 1000 cP | 800 - 1000 cP | Mixed Viscosity |
Aremco Corr-Paint™ CP2070 High Temperature Protective Coating Novolac-Epoxy, Pigment Only Filled Two part, novolac-epoxy with exceptional abrasion adn corrosion resistance for continuous operations to 300°F (150°C) and intermittent use to 400°F (204°C). |
|||
Viscosity | 500 - 1000 cP | 500 - 1000 cP | |
Aremco Quartz-Coat™ 850 High Temperature Specialty Coatings Inorganic, Glass-Ceramic Filled Glass-ceramic, white reflective coating for glass and quartz to 1500°F (816°F) |
|||
Viscosity | 800 - 1000 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
800 - 1000 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080815P1 Silver Flexographic Ink Silver conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and go.. |
|||
Viscosity | 600 - 1000 cP | 600 - 1000 cP | #3 SP @ 60 rpm; RP-0596 |
Solvay RHODOLINE® 643 Surfactant Description :Highly efficient mineral oil based defoamers for flat to gloss paints, quick process foam know down and high in-can persistency.Identification: OIL BASE DEFOAMERAvailable in: North Amer.. |