Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 700 - 900 cP @Temperature 23.0 °C |
700 - 900 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Flex 100 3D Printing Polymer High workability. Meet criteria regarding irritation, sensitisation and cytotoxicity for biological assessment of medical products (DIN ISO 10993)Suitable for the manufacture of flexible objects for.. |
|||
Viscosity | 700 cP | 700 cP | |
Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PNA-157 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 cP @Temperature 30.0 °C |
700 cP @Temperature 86.0 °F |
|
DSM Somos® 7110 Epoxy Photopolymer, Green Parts
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Viscosity | 700 cP @Temperature 30.0 °C |
700 cP @Temperature 86.0 °F |
|
DSM Somos® 7120 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Viscosity | 700 - 527068 cP @Shear Rate 10.0 - 5000 1/s |
700 - 527068 cP @Shear Rate 10.0 - 5000 1/s |
Average value: 221000 cP Grade Count:3 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Viscosity | 700 - 1300 cP | 700 - 1300 cP | |
Huntsman XB 4122 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 330 to 365. Max color is 5.Comments/Applications: Low viscosity, unmodified tough flexible epoxy with excellent workability. For use as a modifier in high solids coa.. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1163 B (SIS) Linear Block Copolymer Description: Kraton D1163 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra.. |
|||
Viscosity | 700 - 1200 cP | 700 - 1200 cP | |
Lucite International Colacryl ® TS1171/1 Acrylic Solution Resin Butyl methacrylate-Methyl methacrylate copolymerThis product is a fairly soft and flexible copolymer with reasonable abrasion resistance. It has good UV resistance and is therefore suitable for outd.. |
|||
Viscosity | 700 cP | 700 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi.. |
|||
Viscosity | 700 cP @Temperature 25.0 °C |
700 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 342-13ACC Single Component Low Viscosity Epoxy Adhesive TRA-BOND 342-13ACC single component, low viscosity epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature in 24 hours .. |
|||
Viscosity | 700 cP @Temperature 25.0 °C |
700 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond FS152C Clear Low Viscosity Epoxy Adhesive TRA-BOND FS152C is a low viscosity epoxy system containing no solvents, cures at room temperature and has excellent flow and wetting characteristics. This two-part adhesive mixes easily and develops.. |
|||
Viscosity | 700 cP @Temperature 25.0 °C |
700 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming EP574 Adhesive Clear unfilled adhesive for thin bond lines.All information provided by Trelleborg Emerson & Cuming |
|||
Viscosity | 700 cP @Temperature 23.0 °C |
700 cP @Temperature 73.4 °F |
|
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy Master Bond Polymer System EP29LPSP is a two component, high performance, modified low temperature heat cured epoxy system specially formulated for cryogenic applications. EP29LPSP is serviceable at.. |
|||
Viscosity | 700 - 1000 cP | 700 - 1000 cP | NOV QC 020 |
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 700 cP | 700 cP | dynamic |
Dow Corning FLUOROGEL® 4-8022 One-part, translucent, heat cure, UV indicator, fuel and solvent resistant.Information provided by Dow Corning |
|||
Viscosity | 700 cP | 700 cP | |
BASF Lupranate® M70L Isocyanate Description: Lupranate® M70L Isocyanate is a solvent-free, medium-viscosity polymethylene polyphenypolyisocyanate. Lupranate M70L Isocyanate, having a higher viscosity than Lupranate M20S, is parti.. |
|||
Viscosity | 700 cP | 700 cP | |
3M Scotch-Weld™ HT700 High Temperature Instant Adhesive 3M™ Scotch-Weld™ High Temperature Instant Adhesives provide superior performance for demanding applications where high temperatures, thermal cycling, or shock resistance is required. HT700 is a me.. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Beijing Ranger Chem SM-815 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Beijing Ranger Chem WSR615 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 700 cP | 700 cP | |
Abatron AboCast 8503-7/AboCure 8503-7 Colorless Epoxy AboCast 8503-7/AboCure 8503-7 is a general purpose, slow hardening, colorless epoxy casting compound with low viscosity. It is similar to the 8503-4 system, but more flexible. Suggested Uses: Trans.. |
|||
Viscosity | 700 cP | 700 cP | |
BASF Lupranate® MP102 Isocyanate Modified MDI Description: Lupranate® MP102 Isocyanate is a liquid, modified short chain prepolymer based on pure 4,4’-diphenylmethane diisocyanate (MDI). Lupranate MP102 Isocyanate is used in conjunction with .. |
|||
Viscosity | 700 cP @Temperature 200 °C |
700 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3500 Polyester, Flake High molecular weight, High toughness, High strength, High elongationUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from produc.. |