Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 250 - 350 cP | 250 - 350 cP | |
ND Industries SuperGlue Ethyl 300 General DescriptionA medium to low viscosity cyanoacrylate which is used for bonding plastics and rubber in various combinations.Meets military spec Mil-A-46050C Type II Class II |
|||
Viscosity | 250 cP @Temperature 30.0 °C |
250 cP @Temperature 86.0 °F |
|
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu.. |
|||
Viscosity | 250 cP | 250 cP | Viscosity of Solution; 5% Styrene |
KKPC KOSYN KBR 710H Polybutadiene Rubber (Low cis BR) Polybutadiene Rubber (Low cis BR)Characteristics: Low cis BR is different in cis content according to the production process and the catalyst. KKPC's low cis LBR has 35% cis content. LBR has hi.. |
|||
Viscosity | 250 cP | 250 cP | |
Shin-Etsu Silicones KE-3421 Silicone, RTV Conformal Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 250 cP | 250 cP | |
Shin-Etsu Silicones KE-3472T Silicone, RTV Conformal Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil OM 250 Methyl Silicone Fluid The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gi.. |
|||
Viscosity | <= 250 cP | <= 250 cP | |
Solvay RHODASURF® L-7/90 Surfactant Chemical Name: NONIONIC EMULSIFIERAvailable in: Asia Pacific, Europe, Latin America and North America Applications: RHODASURF© L 7 90 is an excellent primary nonionic surfactant recommended espec.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | Part B |
Master Bond EP30HT-LO NASA Low Outgassing, Optically Clear Coating Description: Master Bond EP30HT-LO is a moderate viscosity, two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio.. |
|||
Viscosity | 250 cP @Temperature 200 °C |
250 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3250 Polyester, Pellet High elongation type UE3240, Binder paint, Adhesive agentUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as a.. |
|||
Viscosity | 250 cP | 250 cP | |
Von Roll Isola IMI Varnish 73538 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 30°C. Usag.. |
|||
Viscosity | 250 cP | 250 cP | |
Von Roll Isola IMI Varnish 9637 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 29°C. Average solids: 48%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, and bare copper coils... |
|||
Viscosity | 250 - 450 cP | 250 - 450 cP | 542-111 |
Westlake Epolene® N-11P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Information provided by Westlake Chemical |
|||
Viscosity | 250 - 950 cP | 250 - 950 cP | 542-111 |
Westlake Epolene® N-15P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-15P is a low viscosity polypropylene homopolymer powder with a high melt point and excellent hardness. Epolene N-15P is used in color concentrates, toner compounds, and as a p.. |
|||
Viscosity | 250 - 450 cP @Temperature 150 °C |
250 - 450 cP @Temperature 302 °F |
542-111 |
Westlake Epolene® N-21 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-21 is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity m.. |
|||
Viscosity | 250 - 450 cP | 250 - 450 cP | 542-111 |
Westlake Epolene® N-21P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-21P is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity modifier.. |
|||
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 216L01 Clear Low Viscosity Epoxy Adhesive TRA-BOND 216L01 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to g.. |
|||
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
|
Cytec (Conap) RN-1000 / EA-87 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 250 - 325 cP @Temperature 23.0 °C |
250 - 325 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 310M-2 Optically Clear, Flexible Epoxy Material Description: A two component, optically clear, flexible epoxy adhesive designed for optical applications within semiconductor, fiber optic and medical industries. An alternative to EPO-TEK.. |
|||
Viscosity | 250 - 350 cP | 250 - 350 cP | |
Dow CYRACURE™ UVR-6107 Cycloaliphatic Epoxide CYRACURE™ UVR-6107 cycloaliphatic epoxide is a low viscosity base resin. Typical applications include: Metal decoration coatings Overprint varnishes Information provided by Dow |
|||
Viscosity | 250 - 300 cP @Temperature 30.0 °C |
250 - 300 cP @Temperature 86.0 °F |
|
3D Systems Accura® Xtreme Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Viscosity | 250 - 900 cP | 250 - 900 cP | |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |
|||
Viscosity | 250 cP @Temperature 30.0 °C |
250 cP @Temperature 86.0 °F |
|
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |
|||
Viscosity | 250 cP | 250 cP | Part B |
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru.. |