Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 200 cP | 200 cP | |
Resinlab® TL5041 Anaerobic Threadlocking Compound The TL5000 Series anaerobic threadlocking compounds are designed for use in demanding applications to fill the spaces and surface irregularities between tightly mated cylindrical parts. They form a .. |
|||
Viscosity | 200 cP | 200 cP | Fed Std Method 4287 |
Humiseal 1A33LSE Urethane Conformal Coating Humiseal 1A33LSE Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableUL Approval PendingMIL-I-46058C Approval PendingPasses ther.. |
|||
Viscosity | 200 cP | 200 cP | |
KKPC KOSYN KSL 342 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 300 series is a Styrene-Butadiene Latex. Applications: Oil-resistant Foam Rubber, For Impregnation of Tire and Belt Cord, Foam Backing of Textile Go.. |
|||
Viscosity | <= 200 cP @Time 60.0 sec |
<= 200 cP @Time 0.0167 hour |
#60 spindle, 60 rpm; LSY-QB-ID006 |
LG Chemical Lutex 810 SBR Latex Description: Blister Resistance, Ink set off, Sheet Gloss, Coater RunnabilityApplication: Art Paper, Web Offset, Blade Coater and Adhesive coated paperCSA No. 70857-13-5 and 7732-18-5Information pro.. |
|||
Viscosity | 200 cP | 200 cP | |
Silikony Polskie Polastosil M-200 Silicone Rubber Diluent |
|||
Viscosity | 200 - 400 cP | 200 - 400 cP | ASTM D803 |
SK Chemicals SKYTHANE® US230 Magnetic Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | <= 200 cP | <= 200 cP | LV#1; 30 rpm; 540MO3C16 |
Solvay MIRAPOL® SURF-S 210 Surfactant Description: Polymer to be used in alkaline hard surface cleaners and delivering the following benefits through surface modification : spot free, easy cleaning, water sheeting and fast drying. pH 7-.. |
|||
Viscosity | 200 - 300 cP | 200 - 300 cP | Part A |
Master Bond EP30LV Optically Clear, Low Viscosity Epoxy Adhesive Description: Master Bond Polymer System EP30LV is a low viscosity, two component epoxy adhesive for general purpose bonding, coating, sealing and casting formulated to cure at room temperature or mo.. |
|||
Viscosity | 200 cP | 200 cP | dynamic |
Dow Corning SYL-OFF® 7689 CROSSLINKER Syl-Off® 7689 Crosslinker is a solvent-free silicone crosslinker for polyester substrates.Information provided by Dow Corning |
|||
Viscosity | 200 cP | 200 cP | Dynamic |
Dow Corning SYL-OFF® PMCP7689 Crosslinker Syl-Off® 7689 Crosslinker is a solvent-free silicone crosslinker for polyester substrates.Information provided by Dow Corning |
|||
Viscosity | 200 cP | 200 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 400 Coating EtCH-inhibited coating minimized mist at speeds up to 1000 m/min, provides excellent anchorage stability with super calendered kraft and glassine substrates.Information provided by Dow Corning |
|||
Viscosity | 200 cP | 200 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 800 Coating Suitable for lamination with a variety of adhesives, maleate-inhibited coating offers improved thin film stability vs. conventional release coatings and excellent anchorage stability with super cale.. |
|||
Viscosity | 200 cP @Temperature 25.0 °C |
200 cP @Temperature 77.0 °F |
RVT, #1, 10 RPM |
Dow BETAFOAM™ 87155 Polyether / Polyol Blend BETAFOAM™ 87155 is a component used to make high-density, all-water blown rigid polyurethane foam.Information provided by Dow |
|||
Viscosity | 200 cP @Temperature -35.0 °C |
200 cP @Temperature -31.0 °F |
ASTM D2983 |
ExxonMobil Mobil Synturion 6 Mobil Synturion 6 is a premium-quality, synthetic-base fluid specially formulated to meet the demanding lubrication and cooling requirements of mechanical seals --and to maximize seal life. The supe.. |
|||
Viscosity | 200 cP | 200 cP | dynamic |
Dow Corning 409 HS RESIN High-performance coatings; high-temperature applications where low VOC content is required. Used alone or blended with a variety of solvent-based silicone and organic resins. Similar to Dow Corning®.. |
|||
Viscosity | 200 cP | 200 cP | |
Abatron AboCast 8503-6/AboCure 8503-6 Colorless Epoxy AboCast 8503-6/AboCure 8503-6 is a slow hardening, colorless epoxy casting compound with low viscosity used for larger castings. It allows for large castings and offers low viscosity for bubble-free.. |
|||
Viscosity | 200 cP | 200 cP | |
BASF Lupranate® M20HB Isocyanate Description: Lupranate® M20HB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20HB has faster reactivity than polymeric MDI currently used in the wood panel industry. Thi.. |
|||
Viscosity | 200 cP | 200 cP | A Side |
ACC EP RAP-1567 SP-HX EPI Engineered Polymers Silicone Aliphatic Polyurea RAP-1567 SP-HX is a two component 100% solids, no VOC’s, silicone aliphatic polyureas “Powered by ReactAmine® Technology” that was developed for UV stable (colorfast) polyurea applications. This.. |
|||
Viscosity | 200 cP | 200 cP | Uncatalyzed, QM 230F B |
ACC QM 230F QSI Quantum Silicones 30 Durometer Addition Cure Moldmaking Material QM 230F is a two component, room temperature addition cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is a good choice for t.. |
|||
Viscosity | 200 cP | 200 cP | |
BASF Lupranate® M20SB Isocyanate Description: Lupranate® M20SB is a polymeric MDI with a functionality of approximately 2.7. Lupranate® M20SB is a highly efficient, field-proven binder for cellulosic materials in products such as.. |
|||
Viscosity | 200 - 500 cP | 200 - 500 cP | Mixed Viscosity |
Aremco Corr-Paint™ CP2020 High Temperature Protective Coating Urethane, Aluminum Filled This epoxy and urethane based coating is used for producing corrosion and wear resistant barriers to 500 °F. Typical applications include tanks, pipelines, boilers, precipitators, scrubbers, bag ho.. |
|||
Viscosity | 200 - 600 cP | 200 - 600 cP | Mixed Viscosity |
Aremco Corr-Paint™ CP4010 High Temperature Protective Silicone Coating, Aluminum Filled Single part, silicone-based, low viscosity, heat-curable, aluminum-filled sealer offering exceptional moisture resistance to 1100°F (593°C). |
|||
Viscosity | 200 - 500 cP | 200 - 500 cP | |
Epoxyset Epoxibond EB-177 Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
Viscosity | 200 cP | 200 cP | Part A (Isocyanate) |
Resinlab® UR3005 Clear Two Part Urethane Elastomer Resinlab™ UR 3005 Clear is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 Clear provi.. |
|||
Viscosity | 200 cP | 200 cP | Part A (Isocyanate) |
Resinlab® UR3005 Two Part Urethane Elastomer Resinlab™ UR 3005 is a two component, room temperature curing polybutadiene polyurethane casting and potting system. It is designed to cure completely at room temperature. UR 3005 provides excellen.. |
|||
Viscosity | 200 - 500 cP @Shear Rate 50.0 1/s, Temperature 25.0 °C |
200 - 500 cP @Shear Rate 50.0 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080529D7 Carbon Flexographic Ink Carbon conductor ink specifically designed for printing on to polymeric or paper substrates using flexographic printing. Ink can be printed at speeds up to 20m/min, with good line definition and go.. |
|||
Viscosity | 200 - 400 cP | 200 - 400 cP | 15% solution in MEK |
Lubrizol Advanced Materials Pearlstick® 45-40/03 Polycaprolactone based TPU
(discontinued **) TPUs for Solvent-based adhesivesApplications: Automotive, OthersInformation provided by Merquinsa |
|||
Viscosity | 200 - 1500 cP | 200 - 1500 cP | RP-0596 |
Solvay RHODAPON® L-22 STD Surfactant Chemical Name: AMMONIUM LAURYL SULFATECAS: 68081-96-9; 57-55-6Available in: Asia Pacific, Europe, Latin America and North America Applications: The mildness of RHODAPON© L-22 STD is a major reason .. |
|||
Viscosity | 200 cP | 200 cP | |
KKPC KOSYN KSL 210 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 200 series are carboxy metamorphic styrene-butadiene latex. The KSL 200 series has good blending stability with various additives used in paper pro.. |