Dow BETAFOAM™ 87155 Polyether / Polyol Blend

Category Polymer
Manufacturer Dow Chemical
Trade Name BETAFOAM™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow BETAFOAM™ 87155 Polyether / Polyol Blend.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BETAFOAM™ 87155 is a component used to make high-density, all-water blown rigid polyurethane foam.Information provided by Dow
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Solids Content >= 100 %
>= 100 %
Viscosity 200 cP

@Temperature 25.0 °C
200 cP

@Temperature 77.0 °F
RVT, #1, 10 RPM
Thermal Properties Metric English Comments
Flash Point >= 149 °C
>= 300 °F
ASTM D92