Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 150 - 200 cP @Temperature 23.0 °C |
150 - 200 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Cast 100 3D Printing Polymer High reactivity and low viscosity. Excellent dimensional stability.Fulfills the high demands place on digital process chain.Information provided by Genistar. |
|||
Viscosity | 150 - 300 cP @Temperature 25.0 °C |
150 - 300 cP @Temperature 77.0 °F |
Uncured |
Permabond HL138 Anaerobic Retaining Compound Permabond® HL138 is a single component liquid that cures only when in contact with metal parts and oxygen is excluded. The liquid adhesive fills the “air space” between parts and upon cure which .. |
|||
Viscosity | 150 cP | 150 cP | Fed Std Method 4287 |
Humiseal 2A64 Urethane Conformal Coating Humiseal 2A64 Urethane Conformal CoatingHigh moisture resistanceExcellent dielectrical propertiesExcellent chemical resistanceRepairableMIL-I-46058C ApprovedPasses thermal shock test (MIL-I-46058C)F.. |
|||
Viscosity | 150 - 450 cP | 150 - 450 cP | |
Huntsman DY 064 Epoxy Accelerator Mix Ratio with GY 6010 is 5.Comments/Applications: Reduces gel time and cure schedule for adhesives and other fast cure epoxy systems. Tri (dimethylamino methyl) phenol (DMP-30). Dark red, low vi.. |
|||
Viscosity | 150 - 170 cP | 150 - 170 cP | |
Huntsman Matrimid 5292A Resin Color: YellowComments/Applications: 4,4 Bismaleimidodiphenylmethane. Use with Matrimid 5292B to optimize processing, toughness and performance.Data provided by Ciba Specialty Chemicals.Ciba Special.. |
|||
Viscosity | 150 cP | 150 cP | |
KKPC KOSYN KSL 105 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 100 series are carboxy metamorphic styrene-butadiene latexes. They have a soft touch and high adhesive force.Applications: Carpet Backing, Adhesive .. |
|||
Viscosity | <= 150 cP @Temperature 25.0 °C |
<= 150 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil E2 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Viscosity | 150 - 300 cP @Temperature 125 °C |
150 - 300 cP @Temperature 257 °F |
TXAL-A-XX-G-V-005 |
Westlake Epolene® E-14E Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: The Epolene E-14E is a low molecular weight, low density, oxidized polyethylene. The low molecular weight and low softening point contribute to the production of stable, low col.. |
|||
Viscosity | 150 - 300 cP @Temperature 125 °C |
150 - 300 cP @Temperature 257 °F |
TXAL-A-XX-G-V-005 |
Westlake Epolene® E-14EP Oxidized Low Molecular Weight Polyethylene Polymer Description: The Epolene E-14EP is a low molecular weight, low density, oxidized polyethylene powder. The low molecular weight and low softening point contribute to the production of stable, low col.. |
|||
Viscosity | 150 - 700 cP @Temperature 190 °C |
150 - 700 cP @Temperature 374 °F |
542-111 |
Westlake Epolene® E-43 Chemically Modified Polypropylene, Maleation Processed Product Description: Epolene E-43 is a maleic anhydride grafted polypropylene recommended as a coupling agent for polypropylene (PP) composites and for providing slip resistance in floor finish emul.. |
|||
Viscosity | 150 cP | 150 cP | dynamic |
Dow Corning SYL-OFF® SL 2 CROSSLINKER Information provided by Dow Corning |
|||
Viscosity | 150 cP @Temperature 25.0 °C |
150 cP @Temperature 77.0 °F |
|
Cytec Conathane® CC-1194 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Viscosity | 150 cP @Temperature 25.0 °C |
150 cP @Temperature 77.0 °F |
|
Cytec Conathane® CE-1164 (Conap) Polyurethane Dielectric Conformal Coating Dielectric Conformal Coatings for ElectronicsCytec dielectric conformal coatings are the most widely used conformal coatings in industry today for such divergent applications as aircraft avionics, i.. |
|||
Viscosity | 150 - 300 cP @Temperature 23.0 °C |
150 - 300 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 377 High Temperature Epoxy Product Description: EPO TEK®377 is a two component, high Tg, fiber optic grade epoxy adhesive. It is well suited for semiconductor, medical and optical applications.Advantages & Application Notes:.. |
|||
Viscosity | 150 - 250 cP @Temperature 23.0 °C |
150 - 250 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OG603 UV Cure Optical Epoxy Material Description: A single component, low viscosity, UV curable adhesive designed for curing in seconds. It is an all-purpose, general adhesive for optical applications including fiber optic co.. |
|||
Viscosity | 150 cP | 150 cP | |
BASF Lupranate® 224 Isocyanate Description: Lupranate® 224 is a special medium viscosity polymeric MDI containing a high amount of 2,4'-diphenylmethane diisocyanate. The high 2,4'-MDI content will allow for better flow and lon.. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, Moldmaster Green |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, Moldmaster Blue |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, Moldmaster Red |
ACC QM 2128 QSI Quantum Silicones 28 Durometer Condensation Cure Moldmaking Material QM 2128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 150 - 250 cP | 150 - 250 cP | |
Aremco Corr-Paint™ CP4070-S High Temperature Protective Coating, Silicone-Polyester |
|||
Viscosity | 150 - 180 cP @Temperature 30.0 °C |
150 - 180 cP @Temperature 86.0 °F |
|
3D Systems Accura® 60 Plastic for SLA® Systems Simulate the properties and appearance of polycarbonate. For use with solid-state stereolithography (SLA®) systems.ApplicationsTough functional prototypesAutomotive design componentsConsumer electr.. |
|||
Viscosity | 150 - 210 cP @Temperature 25.0 °C |
150 - 210 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PA-28 MDI Isocyanate Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyether-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for p.. |
|||
Viscosity | 150 - 300 cP @Temperature 25.0 °C |
150 - 300 cP @Temperature 77.0 °F |
|
BorsodChem ONGRONAT PE-210 MDI Isocyanate Description of product: It is a 4,4`-diphenyl-methane-diisocyanate and polyester-polyol based prepolymer.Field of application: With suitable polyol blend it can be used as isocyanate component for .. |
|||
Viscosity | 150 cP | 150 cP | Uncatalyzed, Moldmaster Purple |
ACC QM 2125 QSI Quantum Silicones 25 Durometer Condensation Cure Moldmaking Material QM 2125 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent ch.. |
|||
Viscosity | 150 - 250 cP | 150 - 250 cP | |
Aremco Corr-Paint™ CP4020-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 150 - 220 cP | 150 - 220 cP | |
Dow PAPI™ 27 Polymeric MDI PAPI™ 27 polymeric MDI is a polymethylene polyphenylisocyanate that contains MDI. This product has a narrow molecular weight distribution and a high reactivity. Applicable to many foam processes,.. |
|||
Viscosity | 150 cP | 150 cP | |
3M Scotch-Weld™ CA4 Instant Adhesive 3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Fast setting for a variety of plastics and rubbers.Information provided by 3M |
|||
Viscosity | 150 cP | 150 cP | |
KKPC KOSYN KSL 111 Styrene-Butadiene Latex Styrene-Butadiene LatexCharacteristics: KOSYN KSL 100 series are carboxy metamorphic styrene-butadiene latexes. They have a soft touch and high adhesive force.Applications: Carpet Backing, Adhesive .. |
|||
Viscosity | 150 cP @Temperature 80.0 °C |
150 cP @Temperature 176 °F |
|
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy Clear amber, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components t.. |
|||
Viscosity | 150 - 180 cP @Temperature 30.0 °C |
150 - 180 cP @Temperature 86.0 °F |
|
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView .. |