Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1000 - 1600 cP | 1000 - 1600 cP | cPs; 1% solution |
Oceanchem Group Xanthan Gum Oil Drilling Grade Information Provided by Oceanchem Group |
|||
Viscosity | 1300 - 1600 cP @Temperature 71.1 °C |
1300 - 1600 cP @Temperature 160 °F |
|
Northstar Polymers SBA-030 Polyester Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 800 - 1600 cP | 800 - 1600 cP | 25% Toluene Solution at 25°C; BAM 922 |
Kraton® D1161 P (SIS) Linear Triblock Copolymer Description: Kraton D1161 P is a clear, linear triblock copolymer based on styrene and isoprene, with a polystyrene content of 15%. It is supplied from North America in the physical form identified:.. |
|||
Viscosity | 800 - 1600 cP | 800 - 1600 cP | 25% Toluene Solution at 25°C; KM 06 |
Kraton® D1102 J (SBS) Liner Block Copolymer Description: Kraton D1102 J is a clear linear block copolymer based on styrene and butadiene with bound styrene of 30% mass. It is supplied from Japan in the physical form(s) identified below in the.. |
|||
Viscosity | 800 - 1600 cP @Temperature 23.0 °C |
800 - 1600 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® 302-3M Optically Transparent Epoxy Product Description: EPO-TEK® 302-3M is a two component epoxy used for optical, medical, fiber optic, and semiconductor applications. The epoxy is good for adhesive joining, sealing, potting, or as.. |
|||
Viscosity | 800 - 1600 cP @Temperature 23.0 °C |
800 - 1600 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® E4110 Electrically Conductive, Silver Epoxy Product Description: EPO-TEK® E4110 is an electrically conductive, silver-filled epoxy paste. This two component system is designed for low temperature curing from ambient to 80°C, although other.. |
|||
Viscosity | 1000 - 1600 cP | 1000 - 1600 cP | |
Epoxyset Epoxiohm EO-21M-5 Electrically Conductive Epoxy Adhesive EO-21M-5 is an electrically conductive & thermally conductive, silver filled epoxy adhesive. This two component system is designed to be cured at room temperature or the cure can be accelerated by e.. |
|||
Viscosity | 800 - 1600 cP | 800 - 1600 cP | |
Beijing Ranger Chem SM-815CA Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 1200 - 1600 cP | 1200 - 1600 cP | |
Aremco Aremco-Seal™ 529HV High Temperature Specialty Coatings Silicone High viscosity version, transparent silicone sealer with exceptional electrical and moisture resistance to 600°F (316°C). Ideal for use in cartridge heaters. |