Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PAA-033 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-055 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PBA-058 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PPA-019 Polyether Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 cP | 700 cP | |
Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive Resin Technology Group 370 Wire Tacking Fusion™ Cyanoacrylate Instant Ethyl Adhesive |
|||
Viscosity | 700 - 1100 cP @Temperature 25.0 °C |
700 - 1100 cP @Temperature 77.0 °F |
|
Northstar Polymers PNA-157 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 700 cP @Temperature 30.0 °C |
700 cP @Temperature 86.0 °F |
|
DSM Somos® 7110 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7110 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Viscosity | 700 cP @Temperature 30.0 °C |
700 cP @Temperature 86.0 °F |
|
DSM Somos® 7120 Epoxy Photopolymer, Green Parts
(discontinued **) DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Viscosity | 700 cP @Temperature 30.0 °C |
700 cP @Temperature 86.0 °F |
|
DSM Somos® 7120 Epoxy Photopolymer, UV Postcure
(discontinued **) DescriptionDSM Somos® 7120 Photopolymer is a humidity-tolerant, high heat-deflection-temperature, low-curl, high-speed liquid that produces rigid, highly accurate parts. It produces exceptional, u.. |
|||
Viscosity | 700 - 527068 cP @Temperature 230 - 280 °C |
700 - 527068 cP @Temperature 446 - 536 °F |
Average value: 221000 cP Grade Count:3 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Viscosity | 700 cP | 700 cP | KM 06 |
Kraton® D1155 E (SBS) Liner Block Copolymer Description: Kraton D1155 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Europe in the physical form identified: Kraton D1155.. |
|||
Viscosity | 700 - 1200 cP | 700 - 1200 cP | |
Lucite International Colacryl ® TS1171/1 Acrylic Solution Resin Butyl methacrylate-Methyl methacrylate copolymerThis product is a fairly soft and flexible copolymer with reasonable abrasion resistance. It has good UV resistance and is therefore suitable for outd.. |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Huntsman PY 258 Multifunctional Resin Weight per Epoxide (EEW, g/eq) 185 to 196. Max color is 3.Comments/Applications: Provides excellent heat and chemical resistance especially in post bake or heat cured coatings. Chemically modified.. |
|||
Viscosity | 700 cP | 700 cP | Solution Viscosity; ASTM D455 |
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU) Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi.. |
|||
Viscosity | 700 cP @Temperature 25.0 °C |
700 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming EP574 Adhesive Clear unfilled adhesive for thin bond lines.All information provided by Trelleborg Emerson & Cuming |
|||
Viscosity | 700 cP @Temperature 23.0 °C |
700 cP @Temperature 73.4 °F |
|
Master Bond EP29LPSP Low Outgassing, Optically Clear Two Component Epoxy Master Bond Polymer System EP29LPSP is a two component, high performance, modified low temperature heat cured epoxy system specially formulated for cryogenic applications. EP29LPSP is serviceable at.. |
|||
Viscosity | 700 - 1000 cP | 700 - 1000 cP | NOV QC 020 |
Lubrizol ESTANE® 5708F4 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 700 cP | 700 cP | dynamic |
Dow Corning FLUOROGEL® 4-8022 One-part, translucent, heat cure, UV indicator, fuel and solvent resistant.Information provided by Dow Corning |
|||
Viscosity | 700 cP | 700 cP | |
Dow Corning SYL-OFF® 7138 HIGH SPEED CROSSLINKER Syl-Off® 7138 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue, and Syl-Off® 7678 Cr.. |
|||
Viscosity | 700 cP | 700 cP | Dynamic |
Dow Corning SYL-OFF® PMCP7138 High Speed Crosslinker Syl-Off® 7137 High Speed Crosslinker is a 100% active solids crosslinker additive. Recommended for high speed coating conditions where generation of silicone mist is an issue, and Syl-Off® 7678 Cr.. |
|||
Viscosity | 700 cP | 700 cP | dynamic |
Dow Corning 593 FLUID Blend of polydimethylsiloxane and high molecular weight silicone resin.Information provided by Dow Corning |
|||
Viscosity | 700 - 1100 cP | 700 - 1100 cP | |
Beijing Ranger Chem WSR615 Liquid Epoxy Resin Information provided by Beijing Ranger Chemical Co. |
|||
Viscosity | 700 cP | 700 cP | |
BASF Lupranate® MP102 Isocyanate Modified MDI Description: Lupranate® MP102 Isocyanate is a liquid, modified short chain prepolymer based on pure 4,4’-diphenylmethane diisocyanate (MDI). Lupranate MP102 Isocyanate is used in conjunction with .. |
|||
Viscosity | 700 cP @Temperature 25.0 °C |
700 cP @Temperature 77.0 °F |
Uncured |
Permabond HM135 Anaerobic Retainer Permabond® HM135 is a fast curing, medium viscosity anaerobic adhesive for locking and sealing threads and retaining cylindrical components. It gives maximum torque strength on brass or plated bras.. |