Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kraton® D1155 E (SBS) Liner Block Copolymer

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Kraton
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1155 E (SBS) Liner Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Kraton D1155 E is a clear, linear block copolymer based on styrene and butadiene with bound styrene of 40% mass. It is supplied from Europe in the physical form identified: Kraton D1155 ES - supplied as porous pellets dusted with amorphous silicaRegion: North America, Europe, Asia Pacific, Japan, and South America Uses: Kraton D1155 E is used in the modification of polymers and in compounds for technical and footwear applications. It is also used in formulating adhesives, sealants and coatings and as a modifier for bitumen.Applications: Compounding and Personal HygieneInformation provided by Kraton®
Physical Properties Metric English Comments
Volatiles <= 0.10 %
<= 0.10 %
KM 04
Viscosity 700 cP
700 cP
KM 06
Melt Flow 6.0 - 15 g/10 min

@Load 5.00 kg,
Temperature 200 °C
6.0 - 15 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 74

@Time 15.0 sec
74

@Time 0.00417 hour
ASTM D2240
Tensile Strength 28.0 MPa
4060 psi
ISO 37
Elongation at Break 800 %
800 %
ISO 37
Descriptive Properties Value Comments
Content Antioxidant
>0.15%, KM 08
Polystyrene
37-43%, KM 03
Users viewing this material also viewed the following: