Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 6000 cP @Temperature 190 °C |
6000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 4460 Amorphous Polyalphaolefin (APAO) Wire and Cable Grade.Description: Ethylene copolymer and FDA compliantFeatures: Balance high temperature resistance and low temperature flexibilityApplications: Wire and Cable fillings and flooding .. |
|||
Viscosity | 6000 - 8000 cP | 6000 - 8000 cP | |
ND Industries 446 High pressure Sealant Very high strength refrigerant sealant. Maximum solvent resistance |
|||
Viscosity | 6000 - 8000 cP | 6000 - 8000 cP | |
ND Industries StudGrade® 146 Permanent StudGrade HD Threadlocker General DescriptionHigh strength, high viscosity threadlockers for maximum security. Suitable for most applications where disassembly is not required.Typical UsesFasteners over 1" diameter with coa.. |
|||
Viscosity | 6000 cP | 6000 cP | Part B, RVT, #6, 20 rpm; TM R050-12 |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Viscosity | 6000 - 40000 cP | 6000 - 40000 cP | |
Huntsman Araldite GZ 540 X-90 Bisphenol A Epoxy Solution Weight per Epoxide (EEW, g/eq) 233 to 278. Max color is 3.Comments/Applications: GY 6040 - 90% solids in xylene. General purpose bis A epoxy solution for use in 2-package maintenance and architect.. |
|||
Viscosity | 6000 - 16000 cP | 6000 - 16000 cP | |
Huntsman AroCy XU 71787.07 L Cyanate Ester Comments/Applications: Toughened Dicyclopentadiene based cyanate ester resin.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman. |
|||
Viscosity | 6000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
6000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D50706P3 Polymer Dielectric This material is a blue colored screen printable polymer Dielectric, suitable for defining electrode areas and forms a protective layer over the electrode tracking during immersion of the electrode... |
|||
Viscosity | 6000 cP | 6000 cP | |
Shin-Etsu Silicones KE-1204 A Silicone, Potting/Encapsulation RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | <= 6000 cP | <= 6000 cP | #3 SP @ 12 rpm |
Solvay MACKADET® EQ-112 Surfactant Product Description: Mackadet EQ-112 is mild blend of ingredients for the formulation of tear-free baby shampoos. Dilution at 27% in water gives a standard baby shampoo. Uses: Foam Pump, Bubble Bath.. |
|||
Viscosity | 6000 - 8000 cP @Temperature 23.0 °C |
6000 - 8000 cP @Temperature 73.4 °F |
|
Master Bond EP21LV Low Viscosity Two Component Epoxy Master Bond Polymer System EP21LV is a two component, low viscosity epoxy resin system for high performance bonding, sealing, coating, encapsulation and casting. It is formulated to cure readily at .. |
|||
Viscosity | 6000 cP @Temperature 25.0 °C |
6000 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2105 Clear Rigid, Medium Viscosity Epoxy Adhesive TRA-BOND 2105 is a clear, medium viscosity epoxy adhesive which contains no solvents or other additives which can be harmful to the environment or to its users. It has excellent adhesion to glass, c.. |
|||
Viscosity | 6000 cP @Temperature 25.0 °C |
6000 cP @Temperature 77.0 °F |
|
Cytec EN-2541 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Viscosity | 6000 - 7000 cP | 6000 - 7000 cP | |
Epoxyset Epoxibond EB-115 Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |
|||
Viscosity | 6000 cP | 6000 cP | |
Dymax 3094 Solvent-Free Plastic Adhesive Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide .. |
|||
Viscosity | 6000 - 7000 cP @Temperature 35.0 °C |
6000 - 7000 cP @Temperature 95.0 °F |
|
C.O.I.M. DIEXTER® G181 Polyol Polyester Description: The DIEXTER® line of products offers a vast selection of polyol polyesters with different molecular weights and functions. DIEXTER® is sold for the production of polyurethanes in virt.. |
|||
Viscosity | 6000 cP | 6000 cP | |
ACC MM810 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Viscosity | 6000 cP | 6000 cP | |
ACC MM820 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Viscosity | 6000 cP | 6000 cP | "B" component |
ACC QLE 1020 QSI Quantum Silicones 45 Durometer Clear, Addition Cure Elastomer for Coating QLE 1020 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Viscosity | 6000 cP | 6000 cP | |
3M Scotch-Weld™ DP601 Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are gray, rapid, setting, two component polyurethanes. They are packaged as 1:1 ratio liquids in a duo-pack cartridge. With the squeeze of a trigger, the compon.. |
|||
Viscosity | 6000 cP @Temperature -20.0 °C |
6000 cP @Temperature -4.00 °F |
Cold Crank |
ChevronTexaco URSA® SAE 10W-30 Super Plus Texaco Ursa Super Plus SAE 10W-30 delivers value through:One oil for all services, both diesel and gasoline, minimizes the chance of misapplication.Reduced inventory investment — No need to maintai.. |
|||
Viscosity | 6000 cP | 6000 cP | Mixed; TM R050-12 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Viscosity | 6000 cP @Temperature 190 °C |
6000 cP @Temperature 374 °F |
melt viscosity; ASTM D 3236 |
REXtac Rextac® RT 3360 Amorphous Polyalphaolefin (APAO) Modified Bitumen Roofing Grade.Description: Ethylene copolymer and FDA compliantFeatures: High softening pointApplications: Component of modified bitumen roofing systemsOther Properties: Ring and Ba.. |