Dymax 3094 Solvent-Free Plastic Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Dymax Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dymax 3094 Solvent-Free Plastic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Solvent-Free Adhesives for Plastic Assembly in SecondsDymax® Light-Weld® and Ultra 3000 Series UV and UV/Visible Curing Adhesives for plastic assembly provide instant durable bonds to cure a wide variety of engineering plastics. Curing in seconds upon exposure to UV/visible light, these resins are ideal for bonding transparent surfaces and for potting, sealing, and coating applications. Ultra Light-Weld adhesives and sealants cure upon exposure to UV and/or visible light and are perfect for UV blocked and tinted plastics. Light Weld products cure upon exposure to UV light.Environmentally responsible, solvent free adhesives reduce regulatory compliance cost, and encourage worker acceptance of the assembly process.Dymax 3094 Solvent-Free Plastic Adhesive Key Substrates: Polycarbonate (primary), PSU, PU, PVC, Styrene, Acrylic Typical Use: Display cases, shelves
Physical Properties Metric English Comments
Viscosity 6000 cP
6000 cP
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 37.9 MPa
5500 psi
Elongation at Break 300 %
300 %