Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 40000 cP | 40000 cP | RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1320LV Heat Cure Epoxy Conformal Coating Resinlab™ EP1320 and EP1320LV are one part heat cure epoxy conformal coatings. They can also be used as a small mass potting compounds, structural adhesives, or insulating polymer systems where the.. |
|||
Viscosity | 40000 - 60000 cP | 40000 - 60000 cP | |
Lord Adhesives 506 Semi-Flexible, Medium Cure, Medium Viscosity Acrylic Adhesive Lord 500 SeriesLord 500 Series Acrylic Adhesives bond plastics and prepared metals; they offer excellent adhesion to both thermoplastics and thermoset plastics. They are available with varying handi.. |
|||
Viscosity | 40000 - 60000 cP | 40000 - 60000 cP | B |
ITW Plexus Plexusâ„¢ MA300 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive high strength.Information provided by Illinois Tool Works. |
|||
Viscosity | 40000 - 60000 cP | 40000 - 60000 cP | B |
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works. |
|||
Viscosity | 40000 - 60000 cP | 40000 - 60000 cP | B |
ITW Plexus Plexusâ„¢ MA557 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Long working time, non-sagging, excellent g.. |
|||
Viscosity | 40000 - 60000 cP | 40000 - 60000 cP | B |
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works. |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | ASTM D803 |
SK Chemicals SKYTHANE® U0351C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | ASTM D803 |
SK Chemicals SKYTHANE® U1753C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 40000 - 80000 cP | 40000 - 80000 cP | ASTM D803 |
SK Chemicals SKYTHANE® US130J Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Viscosity | 40000 - 50000 cP @Temperature 23.0 °C |
40000 - 50000 cP @Temperature 73.4 °F |
|
Master Bond EP21TDC Toughened, Shock Resistant Two Component Epoxy System Master Bond Polymer Adhesive EP21TDC is a two component epoxy adhesive for general purpose bonding formulated to cure at room temperature or more rapidly at elevated temperatures, with a one-to-one .. |
|||
Viscosity | 40000 cP @Temperature 25.0 °C |
40000 cP @Temperature 77.0 °F |
Mixed (T-F spindle, 10 rpm) |
Tra-Con Tra-Bond 2111 Rigid Epoxy Staking Compound TRA-BOND 2111 is a thixotropic epoxy resin and hardener formulation developed for industrial adhesive, staking, laminating, repair and manufacturing applications where long pot-life, good wetting, n.. |
|||
Viscosity | 40000 cP @Temperature 25.0 °C |
40000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® 5952 Two-Component Easy Mix Ratio Encapsulant Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, .. |
|||
Viscosity | 40000 - 70000 cP | 40000 - 70000 cP | Part A |
Master Bond Supreme 33CLV Two Component, Room Temperature Curing Toughened Epoxy Master Bond Polymer System Supreme 33CLV is a special, room temperature curing, toughened epoxy adhesive/sealant, featuring exceptionally high temperature resistance. This innovative system has outs.. |
|||
Viscosity | 40000 - 70000 cP @Temperature 23.0 °C |
40000 - 70000 cP @Temperature 73.4 °F |
5 rpm |
Epoxy Technology EPO-TEK® T7109-19 Electrically Insulating Epoxy Paste Material Description: A flexible, thermally conductive, electrically insulating epoxy paste designed for low stress and heat dissipation applications. It is an alternative to EPO-TEK® T7109-17, de.. |
|||
Viscosity | 40000 cP | 40000 cP | |
Cotronics 4700 Ultra Temp Adhesive and Casting Epoxy, General Purpose |
|||
Viscosity | 40000 cP | 40000 cP | |
Dymax 9-911 Strain Relief, Wire and Parts Tacking Adhesive High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9-911 Strain Relief, Wire and Parts Tacking AdhesiveRapid, high strength, designed for difficult substrates, resists.. |
|||
Viscosity | 40000 cP @Temperature 177 °C |
40000 cP @Temperature 350 °F |
Typical |
Bostik 6368 Fast Setting EVA Glue Stick Bostik 6368 Fast Setting EVA Glue StickDesigned for packaging. Good temperature resistance. Fast setting. |
|||
Viscosity | 40000 - 90000 cP | 40000 - 90000 cP | Accelerator |
3M Scotch-Weld™ DP110 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP110 Translucent and Gray are two-part epoxy adhesive which combine a fast cure with flexibilityInformation provided by 3M |
|||
Viscosity | 40000 - 70000 cP | 40000 - 70000 cP | |
Aremco Ceramabond™ 516 High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 40000 - 60000 cP | 40000 - 60000 cP | |
Aremco Ceramabond™ 618-N High Temperature Ceramic Adhesive/Paste, Silica Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
Viscosity | 40000 cP | 40000 cP | Part A, RVT, #5, 2.5 rpm; TM R050-12 |
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to.. |