Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 250 - 350 cP | 250 - 350 cP | |
ND Industries 333 Surface Insensitive Instant Superglue Low-medium viscosity for difficult to bond substrates |
|||
Viscosity | 250 - 350 cP | 250 - 350 cP | |
ND Industries SuperGlue Ethyl 300 General DescriptionA medium to low viscosity cyanoacrylate which is used for bonding plastics and rubber in various combinations.Meets military spec Mil-A-46050C Type II Class II |
|||
Viscosity | 250 - 350 cP @Temperature 82.2 °C |
250 - 350 cP @Temperature 180 °F |
|
Northstar Polymers SBA-036 Polyester Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Huntsman HY 9130 Polyamide Approx. H+ equivalent weight 95. Mix Ratio with GY 6010 is 50.Comments/Applications: Low viscosity polyamidoamine for solvent free systems. Good mechanical properties. Adhesives, sealants, floor.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | 10% Toluene Solution at 25°C; KM 06 |
Kraton® G1654 E (SEBS) Linear Triblock Copolymer Description: Kraton G1654 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical .. |
|||
Viscosity | 250 - 1000 cP | 250 - 1000 cP | |
Solvay ALKAMULS® EL 620 Surfactant Description: Castor oil ethoxylate (30 EO) Emulsifier for fats, oils fatty acids and solvents. Maintains stability of oil-in-water emulsions over a wide temperature range as co-emulsifier with an HL.. |
|||
Viscosity | <= 250 cP | <= 250 cP | |
Solvay RHODASURF® L-7/90 Surfactant Chemical Name: NONIONIC EMULSIFIERAvailable in: Asia Pacific, Europe, Latin America and North America Applications: RHODASURF© L 7 90 is an excellent primary nonionic surfactant recommended espec.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | Part B |
Master Bond EP30HT-LO NASA Low Outgassing, Optically Clear Coating Description: Master Bond EP30HT-LO is a moderate viscosity, two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | Part B |
Master Bond EP30HV Optically Clear, High Strength Two Part Epoxy Description: Master Bond EP30HV is a lower viscosity, two component epoxy system for high performance bonding, sealing, coating and potting. It is formulated to cure at room temperature or more rapi.. |
|||
Viscosity | 250 - 400 cP | 250 - 400 cP | Part B |
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to.. |
|||
Viscosity | 250 cP @Temperature 200 °C |
250 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3250 Polyester, Pellet High elongation type UE3240, Binder paint, Adhesive agentUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as a.. |
|||
Viscosity | 250 - 950 cP @Temperature 190 °C |
250 - 950 cP @Temperature 374 °F |
542-111 |
Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer Product Description: Epolene N-15 is a low viscosity polypropylene homopolymer with a high melt point and excellent hardness. Epolene N-15 is used in color concentrates, toner compounds, and as a pi.. |
|||
Viscosity | 250 - 950 cP | 250 - 950 cP | 542-111 |
Westlake Epolene® N-15P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-15P is a low viscosity polypropylene homopolymer powder with a high melt point and excellent hardness. Epolene N-15P is used in color concentrates, toner compounds, and as a p.. |
|||
Viscosity | 250 - 450 cP | 250 - 450 cP | 542-111 |
Westlake Epolene® N-21P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-21P is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity modifier.. |
|||
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 216L01 Clear Low Viscosity Epoxy Adhesive TRA-BOND 216L01 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to g.. |
|||
Viscosity | 250 cP | 250 cP | dynamic |
Dow Corning SYL-OFF® SL 700 COATING Solvent-free, fast curing, provides extremely stable release, excellent bath stability, premium release at low peel speeds, requires catalyst additionInformation provided by Dow Corning |
|||
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
|
Cytec (Conap) RN-1000 / EA-87 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 250 - 350 cP | 250 - 350 cP | |
Dow CYRACURE™ UVR-6107 Cycloaliphatic Epoxide CYRACURE™ UVR-6107 cycloaliphatic epoxide is a low viscosity base resin. Typical applications include: Metal decoration coatings Overprint varnishes Information provided by Dow |
|||
Viscosity | 250 cP | 250 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 700 Coating Information provided by Dow Corning |
|||
Viscosity | 250 - 300 cP @Temperature 30.0 °C |
250 - 300 cP @Temperature 86.0 °F |
|
3D Systems Accura® Xtreme Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco HiE-Coat™ 840-MS High Emissivity Coating, Silicone-Ceramic Filled Silicone-ceramic, black pigmented single component coating for aluminum, brass, copper, and carbon and stainless steel to 1100 °F (593 °C). |
|||
Viscosity | 250 cP | 250 cP | |
3M Scotch-Weld™ MG250-55 UV Medical Grade Light Cure Adhesive 3M™ Scotch-Weld™ Medical Grade Light Cure Adhesive is a single component adhesive that cure to give clear bonds when exposed to appropriate ultraviolet or visible light. It contains a fluorescing .. |
|||
Viscosity | 250 - 900 cP | 250 - 900 cP | |
Aremco Corr-Paint™ CP3015-AL High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Aluminum-ceramic filled coating to 1200°F. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4040-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 250 - 350 cP | 250 - 350 cP | |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |
|||
Viscosity | 250 cP @Temperature 30.0 °C |
250 cP @Temperature 86.0 °F |
|
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |