Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 170000 cP @Temperature 260 °C |
170000 cP @Temperature 500 °F |
melt; 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Americas region. |
|||
Viscosity | 170000 cP @Temperature 260 °C |
170000 cP @Temperature 500 °F |
melt; 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Asia Pacific) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Viscosity | 170000 cP @Temperature 260 °C |
170000 cP @Temperature 500 °F |
melt; 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Cycoloy® CY9650 PC+ABS (Europe-Africa-Middle East) PC+ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Europe-Africa-Middle East re.. |
|||
Viscosity | 170000 cP | 170000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Viscosity | 170000 cP | 170000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Viscosity | 170000 cP @Temperature 260 °C |
170000 cP @Temperature 500 °F |
melt; 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Europe-Africa-Middle East) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat AgingThis data was supplied by SABIC-IP for the Eur.. |
|||
Viscosity | 170000 cP @Shear Rate 60.0 1/s, Temperature 200 °C |
170000 cP @Shear Rate 60.0 1/s, Temperature 392 °F |
|
Noltex Soarnol® ST110 Ethylene Vinyl Alcohol Copolymer Modified DC3203; improved flex crack resistance and thermoformability. Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of n.. |
|||
Viscosity | 170000 cP @Temperature 130 °C |
170000 cP @Temperature 266 °F |
Melt; DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® DIPP-539 is a linear, polycaprolactone-copolester polyurethane with a very high crystallization rate and a very high thermoplasticity level.Applications: PEARLBOND® DIPP-539 can be adde.. |
|||
Viscosity | 170000 - 195000 cP | 170000 - 195000 cP | Average value: 187000 cP Grade Count:6 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Viscosity | 170000 - 1.40e+7 cP @Temperature 200 - 230 °C |
170000 - 1.40e+7 cP @Temperature 392 - 446 °F |
Average value: 1.29e+6 cP Grade Count:11 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Viscosity | 170000 - 1.40e+7 cP @Shear Rate 60.0 - 270 1/s |
170000 - 1.40e+7 cP @Shear Rate 60.0 - 270 1/s |
Average value: 1.29e+6 cP Grade Count:11 |
Overview of materials for Ethylene Vinyl Alcohol (EVOH) This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Alcohol". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Viscosity | 170000 cP | 170000 cP | "A" component |
ACC QLE 1030 QSI Quantum Silicones 27 Durometer Addition Cure Elastomer for Coating
(discontinued **) Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: long pot life, excellent adhesion, 100%solid, fast cure.Applications: fabric or cloth coating. Part of the Amber Chem.. |
|||
Viscosity | 170000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
170000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers KetaSpire® KT-820 SL10 Polyetheretherketone (PEEK) KetaSpire® KT-820 SL10 is a polyetheretherketone (PEEK) based compound designed to offer enhanced lubricity and reduced friction compared to standard PEEK. Unlike other grades formulated for wear.. |
|||
Viscosity | 170000 cP | 170000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® DR51 PBT (Europe-Africa-Middle East) VALOX DR51 is a 15% glass fiber reinforced PBT injection moulding resin with excellent mechanical, thermal and electrical performance. Applications: spotlights, appliance housings, handles. |
|||
Viscosity | 170000 cP | 170000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics Valox® V3500EX PBT (Europe-Africa-Middle East) Unfilled PBT,Flame Retardant, good flow, high elongation at break for Extrusion applications (Monofilaments, Insulation Cables),Electrical Parts and Connectors |
|||
Viscosity | 170000 cP | 170000 cP | |
Elmer's Products Aron Alpha® GEL 10 Cyanoacrylate Adhesive (Industrial Krazy Glue™) Surface insensitive adhesives, ultra-fast setting for porous, soft or tough-to-bond substrates. Series 200TX & Gel: No run, no stringing, excellent gap filling characteristics with good strength on.. |
|||
Viscosity | 170000 cP @Temperature 160 °C |
170000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 170000 cP | 170000 cP | Mixed |
Armstrong A-2/E Epoxy Adhesive This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Ac.. |