Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 8.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Polykemi AB POLYasa 1614F UV-resistant ASA Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE ED80 D40 UV Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics EXTEM VH1003P PEI Copolymer (Asia Pacific) Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Powder version of VH1003. This resin is a Dual-use item and is subject to export control restrictio.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 500R PC (Europe-Africa-Middle East) LEXAN 500R is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and excellent impact pe.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 300 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® ML3290 PC (Europe-Africa-Middle East) LEXAN ML3290 is a high viscosity flame retardant UV stabilized grade especially developed for the extrusion of complex sheet and profiles. LEXAN ML3290 is used in applications where a combination of.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5059 500 Micron LDPE Powder Description: ICOFLO 510-5059 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 315 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 599 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP LUBRICOMP OCL36XXP PPS - Linear (Europe-Africa-Middle East) LNP* LUBRICOMP* OCL36XXP is a compound based on PPS- Linear resin containing PTFE, Carbon Fiber. Added features include : Internally Lubricated, Electrically Conductive . |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2310 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 265 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7503 PC+POLYESTER (Europe-Africa-Middle East) PC-Siloxane copolymer + Polyester alloy, High Impact, Transparent |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GFN1V PPE+HIPS (Europe-Africa-Middle East) NORYL GFN1V is a 10 % glass fibre reinforced material with a HDT/A of 110C according ISO 75. NORYL GFN1V cust spec 1977 has been approved for potable water applications up to 85C by the UK WFBS acco.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL HN731SE PPE+HIPS (Europe-Africa-Middle East) PPE+PS blend. For medical devices and pharmaceutical applications. NORYL HN731SE is an unfilled material, with a Vicat B/120 of 135C according ISO 306. Healthcare management of change, biocompati.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 280 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL N190 PPE+HIPS (Europe-Africa-Middle East) NORYL N190 is an unfilled, flame retardant material with a Vicat B/120 of 105°C according ISO 306. NORYL N190 is V0 at 1.52 mm and 5VA at 3.12 mm according UL94 and halogen free according VDE/DIN.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 360 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Condition E; ASTM D1238 |
A. Schulman LP554-01 Narrow Molecular Weight Homopolymer, High-Density Polyethylene DescriptionLP 554-01 is a narrow molecular weight homopolymer high-density polyethylene exhibiting toughness, rigidity and warpage resistance. ApplicationApplications of LP 554-01 include crates, t.. |
|||
Melt Index of Compound | 8.0 g/10 min | 8.0 g/10 min | Condition L; ASTM D1238 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Melt Index of Compound | 8.0 g/10 min @Temperature 230 °C |
8.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Melt Index of Compound | 8.0 g/10 min | 8.0 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP775-01 Molding Grade, Low Density Polyethylene DescriptionCp 755-01 is a molding grade, low-density polyethylene. ApplicationCP 755-01 meets the specification contained in FDA Regulation 177.1520 for food contact applications.Information provid.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177.. |
|||
Melt Index of Compound | 8.0 g/10 min @Temperature 230 °C |
8.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Melt Index of Compound | 8.0 g/10 min @Temperature 230 °C |
8.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p.. |
|||
Melt Index of Compound | 8.0 g/10 min | 8.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de.. |
|||
Melt Index of Compound | 8.0 g/10 min | 8.0 g/10 min | Condition L; ASTM D1238 |
A. Schulman PP 828-01 Polypropylene Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-01 is a molding grade impact polypropylene. ApplicationThis material meets the FDA Regulation 21 CFR 177.1520 for food contact applications. Information provided by .. |
|||
Melt Index of Compound | 8.0 g/10 min | 8.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 503 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 503 is an injection molding grade olefinic thermoplastic elastomer. This product is recommended for parts requiring flexibility and high impact strength at sub-ambient temp.. |
|||
Melt Index of Compound | 8.0 g/10 min | 8.0 g/10 min | ASTM D1238 |
DuPont Elvax® 550 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Melt Index of Compound | 8.0 g/10 min @Temperature 230 °C |
8.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 828-31 Polypropylene Black Molding Grade Impact Polypropylene DescriptionPolypropylene PP 828-31 Black is a molding grade impact polypropylene.Information provided by A. Schulman. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
|
Axion Polymers Axplas® PS04 0000 Mixed Polystyrene Granules with FR The PS04 series of clean, mixed polystyrene granular chips offers a low-cost option for manufacturers to add post-consumer, engineering polymers to a wide range of products. The polymer mix includes.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTADER® 4503 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4503 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process.LOTADER 4503 is a versatile adhesive for extrusion lamination, des.. |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH TS8038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPHC EP1001F Polypropylene Information provided by Polykemi AB |