Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 260 °C |
20 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 65CI PC/ABS-Blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 260 °C |
20 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 65H MA5 PC/ABS-blend, Low Friction Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PP CCP20020 UV Polypropylene, Mineral Reinforced, UV stabilized Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 265 °C |
20 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CP8930 PC+ABS High heat, PC/ABS for automotive electro plating applications, excellent balance in flow/impact |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC TS20020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH K20020 D Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH T20020 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 265 °C |
20 g/10 min @Load 11.0 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® LG9020 PC+ABS Low Gloss Cycoloy. Available only in natural, to be custom color concentrated and UV stabilized at the molding press. |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 260 °C |
20 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® XP7560 ASA (Europe-Africa-Middle East) GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours. |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 230 °C |
20 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYabs F30 ABS Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC 20000 Polypropylene Copolymer Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH T20020 UV Polypropylene Homopolymer, Mineral Reinforced, UV-Stabilized Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 80 H 4826 TPU-Polyester Introduction: IROGRAN A 80 H 4826 is a thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of this product are excellent mechanical properties and hig.. |
|||
Melt Index of Compound | 20 g/10 min @Load 21.6 kg, Temperature 190 °C |
20 g/10 min @Load 47.6 lb, Temperature 374 °F |
|
Huntsman IROGRAN® A 85 H 4827 TPU-Polyester Introduction: IROGRAN A 85 H 4827 is a thermoplastic polyester polyurethane for injection molding applications. IROGRAN A 85 H 4827 is part of the HUNTSMAN technical injection molding product range .. |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5007 1200 Micron HDPE Powder Description: ICOFLO 510-5007 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 20 g/10 min | 20 g/10 min | ASTM D1238 |
LG Chemical TR-557I Transparent ABS, High Impact, Ice Colored Pellets LG transparent ABS has excellent transparency, impact strength, stiffness, and processability. Since its properties are well balanced, it can be applied widely to a variety of electric and electron.. |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 360 °C |
20 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 360 °C |
20 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Europe-Africa-Middle East) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones.Resin is RoHS compliant. UL94 V0 listing. |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 360 °C |
20 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM UF5011S PEI (Asia Pacific) Enhanced flow, Specialty filtered Polyetherimide (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics and ketones. ECO Conforming. |
|||
Melt Index of Compound | 20 g/10 min @Load 1.20 kg, Temperature 300 °C |
20 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354X PC (Asia Pacific) LNP* Thermocomp* Compound DX11354X is a colorable PC based compound with stable plating and RF performance, colored LDS material solution, good surface and processing window, high impact strength. I.. |
|||
Melt Index of Compound | 20 - 53 g/10 min | 20 - 53 g/10 min | |
Sibur Discar-SL PC/ABS Compositional Polymer Composition material PC/ABS with low viscosity of melting with high shock resistance, thermal and atmospheric resistance for large, thin wall structural parts of automobile interiors. |
|||
Melt Index of Compound | 20 g/10 min @Load 5.00 kg, Temperature 280 °C |
20 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Melt Index of Compound | 20 g/10 min | 20 g/10 min | Condition E; ASTM D1238 |
A. Schulman LP481 Molding Grade High-Density Polyethylene DescriptionLP 481 is a molding grade high-density polyethylene. Information provided by A. Schulman. |
|||
Melt Index of Compound | 20 g/10 min @Temperature 230 °C |
20 g/10 min @Temperature 446 °F |
ASTM D1238 |
Toyobo PELPRENE™ P150B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Melt Index of Compound | 20 g/10 min | 20 g/10 min | 2.16/230; ASTM D1238 |
A. Schulman POLYAXIS® PD8020 Polypropylene DescriptionPolyaxis PD 8020 is a polypropylene designed from rotational molding with a combination of good stiffness and ESCR.NOTE: Physical properties are based on rotationally molded samples from .. |
|||
Melt Index of Compound | 20 g/10 min | 20 g/10 min | ASTM D1238 |
Cheng Yu Plastic PP226 Flame Retardant Polypropylene, Medium Impact |
|||
Melt Index of Compound | 20 - 30 g/10 min @Load 5.00 kg, Temperature 260 °C |
20 - 30 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238, ISO 1133 |
EPICHEM Epiblend PC/ABS nero Polycarbonate/ABS |
|||
Melt Index of Compound | 20 g/10 min | 20 g/10 min | ASTM D1238 |
Amco PRIMATOP HDPE 175953 Injection Molding Polyethylene HDPE 175953 features easy flow, toughness, and high surface gloss. Applications include caps, thin wall parts, and toys.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 230 °C |
20 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH T20040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 20 g/10 min @Load 2.16 kg, Temperature 190 °C |
20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chase Plastics CP Pryme® PE-100LD20M General Purpose Low Density Polyethylene Information provided by Chase Plastics. |