Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
Melt Index of Compound | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1HF PC Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Melt Index of Compound | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1HF PC (Europe-Africa-Middle East) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Melt Index of Compound | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX1132 PC Copolymer (Asia Pacific) Lexan* DMX1132 is a high flow polycarbonate copolymer resin with improved ammonia resistance over regular polycarbonate resin. |
|||
Melt Index of Compound | 36 g/10 min @Load 1.20 kg, Temperature 300 °C |
36 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1HF PC (Asia Pacific) Very high flow, biocompatible polycarbonate for healthcare applications. EtO sterilizable. |
|||
Melt Index of Compound | 36 g/10 min @Load 21.6 kg, Temperature 190 °C |
36 g/10 min @Load 47.6 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 85 P 5350 TPU-Polyester Introduction: IROGRAN A 85 P 5350 is a flame-retardant, halogen-free, polyether based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A 85 P 5350 is par.. |
|||
Melt Index of Compound | 36 g/10 min @Load 2.16 kg, Temperature 260 °C |
36 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Mitsui APELâ„¢ APL5014DP Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melt Index of Compound | 36 g/10 min @Temperature 230 °C |
36 g/10 min @Temperature 446 °F |
ASTM D1238 |
Amco PRIMATOP PP CO 350-20 Impact Polypropylene Copolymer PP CO 350-20 has easy mold flow and excellent dimensional stability. It is used in thin walled injection molded applications.Former A-Top Polymers product; part of Amco product line since 2013. |