Physical Properties Metric English Comments
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 6.40 mm
0.015 in/in

@Thickness 0.252 in
Flow; DAM
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 6.40 mm
0.015 in/in

@Thickness 0.252 in
Transverse; DAM
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66  (Unverified Data**)
Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.00 mm
0.015 - 0.022 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.00 mm
0.015 - 0.022 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® T-662 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.015 - 0.020 cm/cm

@Thickness 3.00 mm
0.015 - 0.020 in/in

@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.00 mm
0.015 - 0.022 in/in

@Thickness 0.118 in
DAM
Toyobo T-661 Nylon 66, Standard Grade (Conditioned)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.
Linear Mold Shrinkage 0.015 - 0.022 cm/cm

@Thickness 3.00 mm
0.015 - 0.022 in/in

@Thickness 0.118 in
Toyobo T-661 Nylon 66, Standard Grade (DAM)
Features: Non-reinforced, Standard GradeInformation provided by Toyobo.
Linear Mold Shrinkage 0.015 cm/cm

@Temperature 240 °C
0.015 in/in

@Temperature 464 °F
ASTM D3392
DuPont™ Nomex® Type 993, 60 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 3.20 mm
0.015 in/in

@Thickness 0.126 in
Transverse; DAM
DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66  (Unverified Data**)
Zytel® FE4200 BK136 is a low die deposit polyamide 66 extrusion resin.Information provided by DuPont Performance Polymers
Linear Mold Shrinkage 0.015 cm/cm

@Thickness 1.27 mm
0.015 in/in

@Thickness 0.0500 in
Transverse; ASTM D955
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Linear Mold Shrinkage 0.015 cm/cm

@Diameter 4.00 mm
0.015 in/in

@Diameter 0.157 in
Normal
DuPont Performance Polymers Delrin® 300ATB BK000 Acetal Homopolymer  (Unverified Data**)
Delrin® 300ATB BK000 is a filled, medium viscosity, toughened acetal homopolymer for injection molding. It is well suited for antistatic applications.Information provided by DuPont Performance Poly..
Copyright © lookpolymers.com All Rights Reserved