Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.0107 cm/cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber Filled, Flame Retardant". Each property range of values re.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0180 cm/cm | 0.00100 - 0.0180 in/in | Average value: 0.0103 cm/cm Grade Count:80 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Linear Mold Shrinkage, Transverse | 0.00110 - 0.0180 cm/cm | 0.00110 - 0.0180 in/in | Average value: 0.00975 cm/cm Grade Count:44 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0180 cm/cm | 0.00200 - 0.0180 in/in | Average value: 0.0113 cm/cm Grade Count:15 |
Overview of materials for Nylon 66/6 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Linear Mold Shrinkage, Transverse | 0.0137 - 0.0180 cm/cm | 0.0137 - 0.0180 in/in | Average value: 0.0146 cm/cm Grade Count:3 |
Overview of materials for Nylon 66, Mineral Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0180 cm/cm | 0.00400 - 0.0180 in/in | Average value: 0.0120 cm/cm Grade Count:9 |
Overview of materials for Nylon 66, Stainless Steel Filled; EMI Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Stainless Steel Filled; EMI Grade". Each property range of values reported is minimum and maxi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00950 - 0.0180 cm/cm | 0.00950 - 0.0180 in/in | Average value: 0.0126 cm/cm Grade Count:4 |
Overview of materials for Nylon 6, MoS2 Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, MoS2 Filled". Each property range of values reported is minimum and maximum values of appropria.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0180 cm/cm | 0.0100 - 0.0180 in/in | Average value: 0.0139 cm/cm Grade Count:101 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |