Polymer Property : Linear Mold Shrinkage, Transverse = 0.0140 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00400 - 0.0140 cm/cm
0.00400 - 0.0140 in/in
Average value: 0.00876 cm/cm Grade Count:14
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45..
Linear Mold Shrinkage, Transverse 0.00600 - 0.0140 cm/cm
0.00600 - 0.0140 in/in
Average value: 0.00811 cm/cm Grade Count:18
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an..
Linear Mold Shrinkage, Transverse 0.00100 - 0.0140 cm/cm
0.00100 - 0.0140 in/in
Average value: 0.00752 cm/cm Grade Count:33
Overview of materials for Nylon 6, Glass Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage, Transverse 0.00590 - 0.0140 cm/cm
0.00590 - 0.0140 in/in
Average value: 0.00989 cm/cm Grade Count:11
Overview of materials for Nylon 6, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a..
Linear Mold Shrinkage, Transverse 0.00560 - 0.0140 cm/cm
0.00560 - 0.0140 in/in
Average value: 0.00853 cm/cm Grade Count:3
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim..
Linear Mold Shrinkage, Transverse 0.00750 - 0.0140 cm/cm
0.00750 - 0.0140 in/in
Average value: 0.0105 cm/cm Grade Count:9
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.00500 - 0.0140 cm/cm
0.00500 - 0.0140 in/in
Average value: 0.00930 cm/cm Grade Count:32
Overview of materials for Nylon 66, Glass/Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage, Transverse 0.00600 - 0.0140 cm/cm
0.00600 - 0.0140 in/in
Average value: 0.00970 cm/cm Grade Count:6
Overview of materials for Nylon 66/6, Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0140 cm/cm
0.0100 - 0.0140 in/in
Average value: 0.0111 cm/cm Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is ..