Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding... |
|||
Linear Mold Shrinkage, Transverse | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Transverse | 0.0027 cm/cm @Time 86400 sec |
0.0027 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Linear Mold Shrinkage, Transverse | 0.0027 cm/cm | 0.0027 in/in | ISO 294-4 |
Solvay Specialty Polymers Kalix® 3850 Polyamide, High Performance (HPPA), 50% Glass Fiber Kalix® 3850 is a 16% bio-sourced, amorphous polyphthalamide (PPA)-based compound with 50% by weight glass fiber reinforcement. This material is uniquely formulated to prevent warpage and flash in.. |
|||
Linear Mold Shrinkage, Transverse | 0.0027 - 0.0061 cm/cm @Thickness 3.20 mm |
0.0027 - 0.0061 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |
|||
Linear Mold Shrinkage, Transverse | 0.0027 - 0.0061 cm/cm @Thickness 3.20 mm |
0.0027 - 0.0061 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Asia Pacific) 40% GR PPE+PP. High elongation. high stiffness. NSF Standard 61 Compliant (color limited). |