Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.023 - 0.024 cm/cm | 0.023 - 0.024 in/in | ASTM D955 |
PolyOne Stat-Tech™ NN-40CF/000 NH FRV0 Natural Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.024 cm/cm @Time 86400 sec |
0.021 - 0.024 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copoly (Asia Pacific) LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Linear Mold Shrinkage, Transverse | 0.021 - 0.024 cm/cm @Time 86400 sec |
0.021 - 0.024 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP Lubricomp KX99792 Acetal Copolymer LNP* Lubricomp* KX99792 is a compound based on Acetal Copolymer resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the .. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Asia Pacific) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.016 - 0.024 cm/cm @Thickness 2.30 - 4.60 mm |
0.016 - 0.024 in/in @Thickness 0.0906 - 0.181 in |
SABIC Method |
SABIC Innovative Plastics Valox® 310SE0 PBT (Europe-Africa-Middle East) VALOX 310SE0 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.024 cm/cm | 0.020 - 0.024 in/in | ISO DIS 294-4 |
Wellman Wellamid® 22L-NBK1 Engineering Grade Nylon 66 Description: Engineering Grade Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.020 - 0.024 cm/cm | 0.020 - 0.024 in/in | ISO DIS 294-4 |
Wellman Wellamid® NY1820-BK1(PTFE) Lubricated, Heat Stabilized Nylon 66 Description: Lubricated, Heat Stabilized Nylon 66Information provided by Wellman. |