Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0140 cm/cm | 0.00400 - 0.0140 in/in | Average value: 0.00876 cm/cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 50% Glass Fiber Filled". Specific grades with glass content between 45.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0140 cm/cm | 0.00600 - 0.0140 in/in | Average value: 0.00811 cm/cm Grade Count:18 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0140 cm/cm | 0.00100 - 0.0140 in/in | Average value: 0.00752 cm/cm Grade Count:33 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Linear Mold Shrinkage, Transverse | 0.00590 - 0.0140 cm/cm | 0.00590 - 0.0140 in/in | Average value: 0.00989 cm/cm Grade Count:11 |
Overview of materials for Nylon 6, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00560 - 0.0140 cm/cm | 0.00560 - 0.0140 in/in | Average value: 0.00853 cm/cm Grade Count:3 |
Overview of materials for Nylon 66/Nylon 6 Blend, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/Nylon 6 Blend, Glass Fiber Filled". Each property range of values reported is minimum and maxim.. |
|||
Linear Mold Shrinkage, Transverse | 0.00750 - 0.0140 cm/cm | 0.00750 - 0.0140 in/in | Average value: 0.0105 cm/cm Grade Count:9 |
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0140 cm/cm | 0.00500 - 0.0140 in/in | Average value: 0.00930 cm/cm Grade Count:32 |
Overview of materials for Nylon 66, Glass/Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Mineral Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0140 cm/cm | 0.00600 - 0.0140 in/in | Average value: 0.00970 cm/cm Grade Count:6 |
Overview of materials for Nylon 66/6, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, Mineral Reinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0140 cm/cm | 0.0100 - 0.0140 in/in | Average value: 0.0111 cm/cm Grade Count:5 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Fiber + PTFE Filled". Each property range of values reported is .. |