Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0110 cm/cm | 0.00200 - 0.0110 in/in | Average value: 0.00592 cm/cm Grade Count:24 |
Overview of materials for Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Syndiotactic Polystyrene (SPS) with Glass or Carbon Fiber". Each property range of values reported is mi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0110 cm/cm | 0.00200 - 0.0110 in/in | Average value: 0.00545 cm/cm Grade Count:17 |
Overview of materials for Liquid Crystal Polymer (LCP), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), Mineral Filled". Each property range of values reported is minimum and max.. |
|||
Linear Mold Shrinkage, Transverse | 0.00900 - 0.0110 cm/cm | 0.00900 - 0.0110 in/in | Average value: 0.00967 cm/cm Grade Count:3 |
Overview of materials for Nylon 66, 10% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc.. |
|||
Linear Mold Shrinkage, Transverse | 0.00190 - 0.0110 cm/cm | 0.00190 - 0.0110 in/in | Average value: 0.00698 cm/cm Grade Count:5 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0110 cm/cm | 0.00100 - 0.0110 in/in | Average value: 0.00708 cm/cm Grade Count:6 |
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value.. |
|||
Linear Mold Shrinkage, Transverse | 0.00330 - 0.0110 cm/cm | 0.00330 - 0.0110 in/in | Average value: 0.00903 cm/cm Grade Count:37 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0110 cm/cm | 0.00500 - 0.0110 in/in | Average value: 0.00792 cm/cm Grade Count:13 |
Overview of materials for Nylon 12, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.0110 cm/cm | 0.00200 - 0.0110 in/in | Average value: 0.00600 cm/cm Grade Count:3 |
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0110 cm/cm | 0.00400 - 0.0110 in/in | Average value: 0.00555 cm/cm Grade Count:47 |
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS)- 40% Glass filled; Molded". Specific grades with glass content between 35% a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0110 cm/cm | 0.00400 - 0.0110 in/in | Average value: 0.00788 cm/cm Grade Count:10 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0110 cm/cm | 0.00800 - 0.0110 in/in | Average value: 0.00958 cm/cm Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Black Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Black Filled". Each property range of values reported is minimu.. |