Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm | 0.0053 in/in | |
Plastcom SLOVAMID 6 GF 30 FRA 5 PA6, 30% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fibre, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6 mm, glow wire at 960°C,.. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm | 0.0053 in/in | |
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra.. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm | 0.0053 in/in | |
Plastcom SLOVAMID 66 GF 15 GB 25 TS PA66, 15% glass fibre, 25% glass beads FeaturesPA 66 chemically reinforced with 15 % glass fibre and with the content of 25% glass beads, thermo stable. Improved anisotropy of shrinkage. The relation of the anisotropy to the mechanical p.. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm | 0.0053 in/in | SABIC Method |
SABIC Innovative Plastics LNP KONDUIT PX09322 PA 6 (Asia Pacific) White colored thermally conductive mineral filled PA6 FR compound |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm | 0.0053 in/in | 60x60x2; 270°C / WZ 80°C; 600 bar; ISO 294-4 |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 cm/cm | 0.0053 in/in | |
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, DRY Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America .. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 - 0.0065 cm/cm @Time 86400 sec |
0.0053 - 0.0065 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 - 0.0065 cm/cm @Time 86400 sec |
0.0053 - 0.0065 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Asia Pacific) LNP* Stat-loy* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant. |