Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 23000 cP @Temperature 25.0 °C |
23000 cP @Temperature 77.0 °F |
at 2 rpm vibration |
Permabond HH131 High Temperature Threadlocker Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for .. |
|||
Viscosity | 23000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
23000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili.. |
|||
Viscosity | 23000 cP @Shear Rate 100000 1/s, Temperature 315 °C |
23000 cP @Shear Rate 100000 1/s, Temperature 599 °F |
|
DSM Arnite® AV2 390 XL PET GF50 50% Glass Reinforced, Low outgassing |