Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 35000 cP @Shear Rate 11200 1/s, Temperature 200 °C |
35000 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne OnFlex™ AW 300-02 Thermoplastic Elastomer (TPE) OnFlex™ AW 300-02 is a non-halogen flame retardant material designed for appliance wire applications. New Product. Commercial specifications have not been established.Purge thoroughly before and af.. |
|||
Viscosity | 35000 cP @Shear Rate 11200 1/s, Temperature 200 °C |
35000 cP @Shear Rate 11200 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne OnFlex™ HFFR 320-01 Thermoplastic Elastomer (TPE) OnFlex™ HFFR 320-01 is a non-halogen flame retardant material designed for flexible power cord insulation and cable jackets. New Product. Commercial specifications have not been established. - Non-.. |
|||
Viscosity | 35000 cP @Shear Rate 1340 1/s, Temperature 200 °C |
35000 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ 9555-1 Thermoplastic Elastomer (TPE) Versaflex™ 9555-1 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Viscosity | 35000 cP @Shear Rate 1340 1/s, Temperature 200 °C |
35000 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ 9555-9 Thermoplastic Elastomer (TPE) Versaflex™ 9555-9 has exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Overmold Adhesion to .. |
|||
Viscosity | 35000 cP @Shear Rate 1340 1/s, Temperature 200 °C |
35000 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Dynaflex™ G2745 Thermoplastic Elastomer (TPE) Dynaflex™ G2745 is designed for injection molding, however, can also be process by extrusion and injection molding. - Easy Processing - Excellent Colorability - Excellent Ozone Resistance and Heat .. |
|||
Viscosity | 35000 cP @Temperature -30.0 °C |
35000 cP @Temperature -22.0 °F |
MRV |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Viscosity | 35000 cP @Shear Rate 5000 1/s, Temperature 190 °C |
35000 cP @Shear Rate 5000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2500 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and tear strength with high impact strength. It.. |
|||
Viscosity | 35000 cP @Temperature -30.0 °C |
35000 cP @Temperature -22.0 °F |
MRV |
ExxonMobil Mobil Clean 10W-40 Motor Oil Mobil Clean Motor Oil is formulated from quality base stocks combined with the most modern performance additives, including an advanced detergent system to provide excellent engine cleanliness. Thes.. |
|||
Viscosity | 35000 cP @Temperature 25.0 °C |
35000 cP @Temperature 77.0 °F |
|
BASF Pluracol® SG-470 Rigid Polyol Description: Pluracol® SG-470 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent .. |
|||
Viscosity | 35000 cP @Temperature 25.0 °C |
35000 cP @Temperature 77.0 °F |
|
BASF Pluracol® SG-450 Rigid Polyol Description: Pluracol® SG-450 polyol is a clear, light colored, sucrose/glycerine polyol. Pluracol SG-450 contains no nitrogen. The high sucrose content with the high hydroxyl number has excellent .. |