Polymer Property : Viscosity = 23000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 23000 cP

@Temperature 25.0 °C
23000 cP

@Temperature 77.0 °F
at 2 rpm vibration
Permabond HH131 High Temperature Threadlocker
Permabond® HH131 is a very high temperature resistant, high strength anaerobic threadlocker and sealant. This material cures in the absence of air between tight fitting metal parts. It is used for ..
Viscosity 23000 cP

@Shear Rate 5000 1/s,
Temperature 190 °C
23000 cP

@Shear Rate 5000 1/s,
Temperature 374 °F
Apparent Dynamic Viscosity
Dow DOWLEX™ 2507 Linear Low Density Polyethylene, Narrow MW Distribution
DOWLEX® 2507 Polyethylene resin is a narrow molecular weight distribution copolymer designed for fast injection molding of thin wall lids without warping. It has demonstrated excellent processabili..
Viscosity 23000 cP

@Shear Rate 100000 1/s,
Temperature 315 °C
23000 cP

@Shear Rate 100000 1/s,
Temperature 599 °F
DSM Arnite® AV2 390 XL PET GF50
50% Glass Reinforced, Low outgassing