Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | Base Oil; ASTM D445 |
Nye Lubricants 702A-EP (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 220 Mobil DTE PM Ashless Mobil DTE PM Ashless products are high-performance, environmentally friendly lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provi.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 220 Mobil DTE PM Series Mobil DTE PM Series products are high-quality, high-performance lubricants specifically designed for demanding industrial paper machine circulating systems. They are engineered to provide exceptiona.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 222 Special Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil Gargoyle Arctic 230 SHC 200 Series Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil Mobil Glygoyle 220 Mobil Glygoyle Series lubricants are supreme performance gear, bearing and compressor oils designed to provide outstanding benefits in terms of efficiency, long oil life, and equipment protection. T.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil Unirex EP Unirex EP 2 is a premium-quality mineral-oil grease. The advanced lithium-complex soap with a combination of an ISO 220 base oil and performance enhancing polymer technology provides excellent high.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 220 Mobilgear SHC Series The Mobilgear SHC Series lubricants are heavy-duty gear oils primarily designed for all kinds of enclosed gearing as well as plain and rolling element bearings. They are formulated from wax-free pol.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | |
ChevronTexaco Aquagear® EP 220 Texaco Aquagear EP oils deliver value through:Long equipment life — Effective sulfur-phosphorus extreme-pressure additives provide high film thickness that protects gear teeth from wear and prematu.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | See Note 3. |
ChevronTexaco EP 1 Aluminum Complex Texaco Aluminum Complex EP 1 is manufactured using selected, high viscosity base oils, EP additives, rust and oxidation inhibitors. It has a high dropping point, which reduces the need for addition.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ChevronTexaco Gear Compounds EP J, ISO 220 FeaturesChevron Gear Compounds EP J are multipurpose gear lubricants.They are formulated with highly refined, high viscosity
index paraffinic base oils and a new generation sulfurphosphorus additive.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ChevronTexaco ISO 220 AIO FeaturesChevron AIO (Chevron Authentic Industrial Oils) provide rust protection, oxidation inhibition, and foam suppression.Chevron AIO are good quality lubricants for any application not requiring .. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | See Note 3. |
ChevronTexaco Marfak® Multipurpose NLGI Grade 2 Texaco Marfak Multipurpose delivers value through:Good water resistance — Provides lubrication in the presence of water.Good corrosion protection — Inhibited to protect gear and bearing surfaces.G.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ChevronTexaco Regal® 220 R&O Texaco Regal R&O oils deliver value through:Prolonged oil service life — Excellent oxidation stability provided by the multi-component inhibitor system resists oil breakdown during exposure to high.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 220 Mobilith SHC PM Mobilith SHC PM greases are supreme performance products designed specifically for severe paper machine applications, including extreme temperature environments and exposure to different qualities o.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 220 Mobilith SHC Series Mobilith SHC Series greases are supreme performance products designed for a wide variety of applications at extremes of temperature. They combine the unique features of synthetic base fluids with th.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 221 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 222 Mobilgrease FM Mobilgrease FM 221 and FM 222 are high performance multi-purpose products designed specifically for the lubrication of food processing machinery. Mobilgrease FM 221 and FM 222 are formulated with co.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 222 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 223 Mobilgrease XHP Series Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outper.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 630 Mobilgear 600 Series The Mobilgear 600 Series are extra high performance gear oils having outstanding extreme pressure characteristics and load-carrying properties, intended for use in all types of enclosed gear drives .. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil Enmist EP 220 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil Mobil 1 Synthetic Grease Mobil 1 Synthetic Grease is an NLGI No 2 high-performance grease which combines a synthetic base fluid with a lithium complex soap thickener. The thickener system provides a high dropping point, whi.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil Spartan EP 220 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D-445 |
ConocoPhillips ANDEROL® HTC Chain & Way Fluid, Synthetic Food Grade ISO 220 Description: ANDEROL HTC Fluids are made from synthetic hydrocarbons (PAO) and special additive packages which allow them to meet the former H-1 approval requirements of the USDA where incidental fo.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | |
ConocoPhillips Hydroclear® 220 Wet Gas Compressor Fluid ISO 220 Description: Conoco Hydroclear® Wet Gas Compressor Fluid is designed to lubricate rotary screw and reciprocating compressors in natural gas service. Conoco's high-quality, hydrocracked base oil.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil 220 Mobilgear SHC XMP Series Mobilgear SHC XMP Series supreme performance, fully synthetic industrial gear oils designed to provide optimum equipment protection and oil life even under extreme conditions. Mobil polyalphaolefin .. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil Enmist EP 220 Esso ENMIST EP is a family of premium quality industrial lubricants designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. ENMIST EP mist .. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ExxonMobil Spartan EP 220 Exxon SPARTAN EP lubricants are a family of premium quality extreme pressure gear lubricants. They are formulated with high quality mineral oils, which help reduce sludge formation and oil thickenin.. |
|||
Kinematic Viscosity at 40°C (104°F) | 220 cSt | 220 cSt | ASTM D445 |
ChevronTexaco Regal® 220 Texaco Regal oil delivers value through:Long lubricant life provided by good natural thermal and oxidation stability.Good demulsibility, which assures good lubricant, film strength and reduced wear .. |