ExxonMobil 222 Special Mobilgrease XHP Series

Category Fluid , Lubricant , Lithium Gellant
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil 222 Special Mobilgrease XHP Series.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mobilgrease XHP Series products are extra high performance lithium complex greases intended for a wide variety of applications and severe operating conditions. These greases were designed to outperform conventional products by applying leading edge, proprietary, lithium complex manufacturing technology. They are based on high quality paraffinic mineral oils and are manufactured and formulated to provide excellent high temperature performance with good adhesion, structural stability and resistance to water contamination. These greases have a high level of chemical stability and offer excellent protection against rust and corrosion. The greases feature high dropping points and maximum recommended operating temperature for the Series is 175°C.Mobilgrease XHP greases are used in a wide range of equipment including industrial, automotive, construction and marine applications: Mobilgrease XHP 222 is recommended for industrial and automotive antifriction bearings, chassis components, universal joints and disc brake wheel bearings. It finds particular application in passenger cars, light trucks, taxi fleets and farm equipment. It is also recommended for marine, paper mill, sugar mill and mining applications; Mobilgrease XHP 461 is recommended for construction and mining equipment, paper and steel mills and other heavy-duty applications; Mobilgrease XHP 222 Special is used in chassis components, clutch bearings, ball joints of suspension and steering systems in all kinds of passenger cars, trucks, farm tractors, contractor, construction, earth-moving, and mobile equipment. Contains molybolenum disulphide that provides protection from wear under shock loads and fretting conditions.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 220 cSt
220 cSt
ASTM D445
Oxidative Stability 100 hour
100 hour
Pressure Drop of 35 kPa; ASTM D942
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Weld Load 315 kg
695 lb (mass)
ASTM D2596
Four Ball Wear 0.500 mm
0.0197 in
ASTM D2266
Penetration -8.00
-8.00
Penetration Consistency Change, Roll Stability, mm/10; ASTM D1831
280
280
Worked, 25°C; ASTM D217
Timken Test 20400 g
45.0 lb
Thermal Properties Metric English Comments
Dropping Point 280 °C
536 °F
ASTM D2265
Descriptive Properties Value Comments
Color grey-black
Copper Strip Corrosion, ASTM D4048 1A
Corrosion Prevention, ASTM D1743 pass
Emcor/SKF Water Wash Test, IP 220 0
Soap/Thickener Type lithium complex
Water Spray Resistance, ASTM D4049, % Spray-off 15
Water Washout, ASTM D1264, wt% 5
@ 79°C