ChevronTexaco Regal® 220

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Regal® 220.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Texaco Regal oil delivers value through:Long lubricant life provided by good natural thermal and oxidation stability.Good demulsibility, which assures good lubricant, film strength and reduced wear through quick water separation.Good air release by the foam inhibitor hastening the release of foam and entrained air.Texaco Regal oils provide protection due to its good natural thermal and oxidation stability, as well as foam suppression.Texaco Regal oils are good quality lubricants for any application not requiring R&O, antiwear, or extreme pressure protection.The thermal and oxidation stability also reduces the possibility of oxidation deposits or the generation of acidic material from oxidation.It has good demulsibility characteristics allowing quick release of moisture. It minimizes entrained air which otherwise could result in low lubricant film strength between moving parts and pump cavitation.Texaco Regal oils can also be used as a general-purpose machine oil for shop use wherever a highly refined petroleum oil with good demulsibility and air release, but without other additives, is used. They can be used to lubricate gears, pinions, and bearings in industrial mills. They can also be used to lubricate geared motors, and has applicability in steel mills, rubber rolling mills, and roller chains.Do not use in breathing air apparatus or medical equipment.Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 220623; MSDS Number: 8607
Physical Properties Metric English Comments
API Gravity 28.5 °
28.5 °
ASTM D287
Viscosity Measurement 97
97
Viscosity Index; ASTM D2270
Saybolt Viscosity at 100°F 1163 SUS
1163 SUS
ASTM D445
Saybolt Viscosity at 210°F 96.8 SUS
96.8 SUS
ASTM D445
Kinematic Viscosity at 40°C (104°F) 220 cSt
220 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 19 cSt
19 cSt
ASTM D445
Thermal Properties Metric English Comments
Pour Point -15.0 °C
5.00 °F
ASTM D97
Flash Point 294 °C
561 °F
ASTM D92