Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Mobil 1 Synthetic Grease

Category Fluid , Lubricant , Lithium Gellant
Manufacturer ExxonMobil
Trade Name Mobil 1
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Mobil 1 Synthetic Grease.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Mobil 1 Synthetic Grease is an NLGI No 2 high-performance grease which combines a synthetic base fluid with a lithium complex soap thickener. The thickener system provides a high dropping point, while additives impart optimum extreme-pressure properties and excellent resistance to water wash, and outstanding protection against rust and corrosion. Mobil 1 Synthetic Grease has excellent structural stability and low-temperature pumpability, making it an outstanding automotive grease.Mobil 1 Synthetic Grease meets the requirements of the National Lubricating Grease institute (NLGI) performance classification GC-LB. It is recommended for automotive applications at both high and low temperatures. It is particularly suited for applications such as disc brake wheel bearings, ball and steering joints, and universal joints. It will provide outstanding bearing protection under heavy loads at any highway speed, and where moisture or condensation is a factor.
Physical Properties Metric English Comments
Kinematic Viscosity at 40°C (104°F) 220 cSt
220 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 23.8 cSt
23.8 cSt
ASTM D445
Mechanical Properties Metric English Comments
Four Ball Extreme Pressure, Load Wear Index 45
45
Four Ball Extreme Pressure, Weld Load 250 kg
551 lb (mass)
ASTM D2596
Four Ball Wear 0.400 mm
0.0157 in
ASTM D2266
Penetration 280
280
Worked x 60 strokes; ASTM D217
295
295
Worked x 10000 strokes; ASTM D217
305
305
Worked x 100000 strokes; ASTM D217
Timken Test 20400 g
45.0 lb
Thermal Properties Metric English Comments
Dropping Point 288 °C
550 °F
ASTM D2265
Descriptive Properties Value Comments
Color red
Corrosion Prevention, ASTM D1743 pass
Emcor/SKF Water Wash Test, IP 220 0
Soap/Thickener Type lithium complex
Structure smooth; slight tack
Water Washout, ASTM D1264, wt% 6
@ 79°C