Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D792 |
S&E Specialty Polymers G-95-045G PVC Application: Matt finish PVC extrusion compound.Information provided by S&E Specialty Polymers |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | NBR NM-IEC 60811-1-3 |
Karina 32/34-FC-LMP (SDB) Orange Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 46/9-G Pearl Color Concentrate for PVC Color concentrate recommended for application in PVC compounds for general purposes injection. Recommended to use 2%.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 700-48/1-B-IS-BZ. Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 802-06/77-Y-BZ Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 804-06/115-CRM Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 804-48/1-CRM Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | NBR NM-IEC 60811-1-3 |
Karina 809D48/1-C-IS-LMP Black PVC Compound Heavy metal free PVC compound recommended for extrusion of coaxial cables jacket. Also recommended for extrusion of automotive flexible tube. Working temperature range: -40°C to +80°C.Inform.. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 810-06/115-CRB Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 810-37/3-CRB Ocher PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 822-18/599-CRB-LMP Gray PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 900D06/366-B-IS-BZ Blue PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina 909D48/1-C-IS-LMP Black PVC Compound Heavy metal free PVC compound, flexible at low temperatures, recommended for automotive wires and cables recovering.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 36/210-GEN Green Brown (SP31456) for PVC Recommended usage from 2% to 3% on crystal PVC compoundInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 81-10/43-CR White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 813-35/1-Y-SN-ERYB Ivory PVC Compound Tin stabilized PVC compound recommended for extrusion of interior furnishing boards and profiles. Developed for Teknaform Canada.Information provided by Karina Indústria e Comércio de Plás.. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 818-10/23-CRM-AS White PVC Compound UV. protection addedInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 820-18/100-CR Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 822-10/148-CRB-LMP White PVC Compound Heavy metal free PVC compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 830-18/99-CRB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 835-35/1-ERYB-AS Ivory PVC Compound Rigid ivory PVC compound with anti-UV protection, developed for extrusion profile under 8700x0220 sample analysis.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 839-10/19-Y-CR White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 854-18/99-CRB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.35 - 1.39 g/cc | 1.35 - 1.39 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom AM-05495 PVC Compound The polycom AM series are designed for the covering of wires for the production of fences. They are available in different colors and all provide excellent UV light and microorganisms resistance. A.. |
|||
Specific Gravity | 1.35 - 1.39 g/cc | 1.35 - 1.39 g/cc | ASTM D-792 |
Axiall 67441 Wire & Cable Flexible PVC 90°C rated, non-lead stabilized, inner/outer jacketing compound meets -40°C low temp impact and FT4 flame requirements in Teck 90 cables. Low acid gas 12%-13% per CSA test methods. Meets CSA 22... |
|||
Specific Gravity | 1.35 - 1.39 g/cc | 1.35 - 1.39 g/cc | ASTM D-792 |
Axiall 8950 Moldings & Extrusions Flexible PVC General purpose semi-rigid extrusion compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.35 - 1.39 g/cc | 1.35 - 1.39 g/cc | ASTM D-792 |
Axiall 19871 Wire & Cable Flexible PVC Non-lead stabilized, 105°C rated insulation compound with very good migration and oil resistance. Recommended for toner resistance applications.Information provided by Georgia GulfGeorgia Gulf bec.. |
|||
Specific Gravity | 1.35 - 1.39 g/cc | 1.35 - 1.39 g/cc | ASTM D-792 |
Axiall 22900 Coax & Telecom Flexible PVC Riser jacket over PVC and FRPE.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.33 - 1.39 g/cc | 1.33 - 1.39 g/cc | ASTM D 792 |
Karina E 843-18/302-CRM Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.35 - 1.39 g/cc | 1.35 - 1.39 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom AM-440495 PVC Compound The polycom AM series are designed for the covering of wires for the production of fences. They are available in different colors and all provide excellent UV light and microorganisms resistance. A.. |