Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.74 g/cc | 1.74 g/cc | |
Premix Premi-Glas® 1266 (Injection Compression Molded) Glass Reinforced TMC Description: Premi-Glas® 1266 is a glass reinforced thermoset molding compound designed for automotive under the hood applications. Key features and benefits: Designed for Injection or Injection/Co.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | |
Premix Premi-Glas® 1268 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1268 is a fiberglass reinforced thermoset thick molding compound for composite power train applications such as valve covers and timing gear covers.Key features and benefits are:Ideal f.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | ASTM D792 |
Quantum Composites QC-7753 50% Glass Fiber Reinforced Polyester SMC QC-7753 is a polyester engineered structural composite molding compound that is designed for applications requiring high strength, fire retardant properties, and resistance to elevated temperatures... |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit Consil®-A 897 Silver-Aluminum Filled Silicone Elastomer Description: CONSIL-A is a silicone or fluorosilicone elastomer filled with silver-plated aluminum particles designed to achieve maximum electrical conductivity. CONSIL-A provides high shielding eff.. |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit NC-Consil® 751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Specific Gravity | 1.74 - 2.26 g/cc | 1.74 - 2.26 g/cc | ASTM D792 |
Parker Chomerics Tecknit NC-Consil® FR751 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 1301-7836 PPS, linear, with glass fiber, lubricant modified Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Low warpage, isotropic shrinkage characteristics.Chemical and hydrolysis resistance parts.High dim.. |
|||
Specific Gravity | 1.74 - 1.80 g/cc | 1.74 - 1.80 g/cc | ASTM D 792 |
Karina 18/97-RG-GE (CS) Gray Color Concentrate for PVC Heavy metal free color concentrate recommended for application in electrical wire and cable PVC compounds. Also suitable for pigmentation of flexible and rigid PVC compounds for general purposes. .. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | |
MTI ThermoStran® TPU-60G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Specific Gravity | 1.74 - 1.77 g/cc | 1.74 - 1.77 g/cc | ASTM D792 |
Shanghai Ofluorine D-1 PVDF Lithium Ion Battery Binders (DF-2) Description: D-1 PVDF Powder has good solubility in some solvent, it is more suitable for lithium ion battery industry as binder. D-1 PVDF is a homopolymer with high dielectric constant, which shows.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | |
Silberline EternaBrite® Premier 351-PA EternaBrite® Premier pigments are leafing aluminum pigment pastes carried in isopropyl alcohol. These grades are based on lenticular flake geometry and offer enhanced leafing properties in solven.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® VB-5400G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | Absolute Drying; ASTM-D792 |
Toyobo GLAMIDE® TY-791HT 6T-Nylon GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Specific Gravity | 1.74 g/cc @Temperature 25.0 °C |
1.74 g/cc @Temperature 77.0 °F |
|
Dow Corning LSPRD13 SILICONE MASTERBATCH RED Information provided by Dow Corning |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | at 25°C |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | at 25°C |
Daikin NEOFLON RP-4040 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | at 25°C |
Daikin NEOFLON RP-5000AS EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | Part A |
Epoxy Technology EPO-TEK® H20S Electrically Conductive, Silver Epoxy for Die Stamping Product Description: EPO-TEK® H20S is a modified version of EPO-TEK® H20E, designed primarily for die stamping and dispensing techniques for chip bonding. EPO-TEK®H20S is a highly reliable, two .. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | ASTM D792 |
Asahi Glass Fluon® C-88AXP ETFE Fluororesin A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | ASTM D792 |
Asahi Glass Fluon® ETFE A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | Method A; ASTM D792 |
LNP Konduit® OTF-202-10 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically Conductive, Thermally ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; h.. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® V9561 PET (Europe-Africa-Middle East) Flame retardant PET, 30% Glass fiber filled. Offering a good balance in CTI , GWIT , High Heat and mechanical performances. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | ASTM D792 |
E-Polymers SEPAZ® C240GM 40% Glass Fiber/Mineral Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |
|||
Specific Gravity | 1.74 g/cc | 1.74 g/cc | ASTM D792 |
E-Polymers SEPAZ® C245GP 45% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |