Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100-15 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100-15 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1200H-22 Fiberglass Reinforced Thermoset SMC Premi-Glas® 1200H-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose and HVAC applications requiring thermal stability and stiffness.Key features and benefits are:Go.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-20 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-20 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 1240-25 Fiberglass Reinforced Thermoset Thick Molding Compound Premi-Glas® 1240-25 is a fiberglass reinforced thermoset Thick Molding Compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-22 CRSX Polyester BMC Premi-Glas® 2103-22 CR-SX is a 22% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-22 CR-SX-HT Fiberglass Reinforced Thermoset BMC Premi-Glas® 2103-22 CR-SX-HT is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL .. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-15 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-15 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2203-22 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-22 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 3200-22 Fiberglass Reinforced SMC Description: Premi-Glas® 3200-22 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di.. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
Quadrant EPP Techtron® PSGF PPS - Compression Molded 40% Glass Reinforced Polyphenylene Sulfide (ASTM Product Data Sheet) |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
Quantum Composites QC-8850 43% Glass Fiber Reinforced Polyester Hybrid SMC QC-8850 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and .. |
|||
Specific Gravity | 1.70 - 1.80 g/cc | 1.70 - 1.80 g/cc | ISO 1183 |
Raschig Group MELOPLAS® 3025 MF Cellulose-reinforced and inorganically filled MF molding compound in white and colored shades. High surface hardness, good UV and heat stability, very good resistance to chemicals - also to foodstu.. |
|||
Specific Gravity | 1.70 - 1.85 g/cc | 1.70 - 1.85 g/cc | |
Premix Premi-Glas® 2103-10 CRSX Polyester BMC Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U.. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ISO 1183 |
Lanxess Pocan® T 7141 000000 PET + PBT, 40% Glass Fiber/Mineral PET + PBT, 40% glass fibers/mineral, injection molding, improved flowability, high thermal dimensional stabilityInformation provided by LANXESS. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | |
Shin-Etsu Silicones FE-281U Fluorosilicone Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® V8280SF PBT+PET High Modulus, PBT+PET, 40% Glass Reinforced, Mold Release, Super High Flow |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ASTM D792 |
Cheng Yu Plastic NG1600S Nylon 66, 60% Glass Fiber Reinforced |
|||
Specific Gravity | 1.70 - 1.90 g/cc | 1.70 - 1.90 g/cc | IEC 1212-2 8.1 |
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech.. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | ETFE film property; ASTM D792 |
Arlon 25188T010 Silicone Rubber/Laminated ETFE Film Liner: 3 mil PTFE coated fiberglass; Side 1: uncured silicone rubber; Substrate: laminated ETFE film, treated for adhesion |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | Part B; TM R050-16 |
Resinlab® EP1200LV Casting Resin Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an.. |
|||
Specific Gravity | 1.70 g/cc | 1.70 g/cc | 73°F; ASTM D792 |
Matrixx Group 80M7451 45% Glass/Mineral Filled PET
(discontinued **) Data provided by The Matrixx Group, formerly RePlas. |