Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
Ovation Polymers RIGITRON 30525 GF FR PET, 25% Glass Reinforced PET – 25% Short Glass Fiber Reinforced with Flame retardant. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to AS.. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
PolyOne Edgetek® PS-15GF-25MN/000 Polybutylene Terephthalate (PBT), Glass/Mineral Filled
(discontinued **)< Description/Features:Glass/Mineral ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ISO 1183 |
Lehmann & Voss LUVOCOM® 20-8261 Polyphthalamide, with carbon fiber, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Improved friction and wear.. |
|||
Specific Gravity | 1.63 g/cc @Temperature 23.0 °C |
1.63 g/cc @Temperature 73.4 °F |
ASTM D792 |
Kingfa PBT-RG30 Flame Retardant, 30% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesOutstanding electrical propertiesGood heat resistanceApplications:Injection moldingConnectorsRelayBobbins, plugsE & E partsInformation.. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
LG Chemical LUMID GP2301BF PA 66+GF30%, Flame Retardant Feature: Injection Molding, PA 66+GF30%, Flame RetardantApplication: IT/OA (Micro Switch, ConnectorCAS No. 32131-17-2, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Che.. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East) 30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
SABIC Innovative Plastics Valox® 420SE0U PBT PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | |
Shin-Etsu Silicones SFX-14036AU Fluorosilicone Elastomer Product Description Shincor SFX14036AU is normal 75 Durometer fluorosilicone compounds. It is designed to process well in molding applications. Product Features: Excellent fuel and solvent resistanc.. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | |
Silberline Extra Fine "P" Extra Fine "P" is a standard polished grade; class "A", fine, leafing aluminum pigment carried in mineral spirits.Applications: Trade & Maintenance |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | |
Silberline Extra Fine "T" Extra Fine "T" is a standard polished grade; class "A", fine, leafing aluminum pigment carried in mineral spirits.Applications: Trade & Maintenance |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
Samsung Cheil Industries Infino® VB-5300G PBT, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
Teknor Apex Fireguard® 910L16-C6-NL1 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: Flame Retardant; Low Smoke Emission Uses: Plenum Cable Jacketing Wire Types: CL2P; CL3P; CMP; FPLP; MPP; OFNP Agency Ratings: NEC Article 725; NEC Article 760; NEC Ar.. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
A. Schulman VOLOY™ 461 Glass Reinforced, Flame Retardant PBT Alloy Information provided by A. Schulman. |
|||
Specific Gravity | 1.63 g/cc @Temperature 25.0 °C |
1.63 g/cc @Temperature 77.0 °F |
|
Dow Corning LSPRD10 SILICONE MASTERBATCH RED Information provided by Dow Corning |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
A. Schulman POLYBATCH™ Grey 8035 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 8035 is a grey color concentrate based in polyethylene. This concentrate was designed to provide opacity and color in polyolefin film and molding applications. POLYBATCH® 8.. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | Mixed; TM R050-16 |
Resinlab® EP1200LV Casting Resin Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an.. |
|||
Specific Gravity | 1.63 g/cc | 1.63 g/cc | ASTM D792 |
PolyOne Edgetek® AT-30GF/000 Acetal-Copolymer, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |